Investigation on Microstructure of Steel-bonded Molten Cemented Carbides AITranslate

School of Materials Science and Engineering, Beijing University of Technology;School of Materials Science and Engineering, Beijing University of Technology;School of Materials Science and Engineering, Beijing University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Analysis is made of the structure of WC based steel bonded molten and annealed cemented carbides and study was made of the influence of different carbon addition on the structure,The results showed that WC is not present in the structure of molten steel bonded cemented carbide.Proper increase of carbon or WC content and annealing will help improve the improper structures and WC reduction.

KeyWords AITranslate

steel bonded cemented carbide melting C content cemented carbide compound annealing treatment.

1尤显卿,郑玉春,朱晓勇,马建国,黄曼平.电冶熔铸WC-Co/钢复合材料组织和性能的研究[J].中国稀土学报,2003,21(z1):133-136. 被引量:4

2尤显卿,马建国,宋雪峰,任昊,黄曼平.电冶熔铸WC/钢复合材料中WC的溶解行为[J].中国有色金属学报,2005,15(9):1363-1368. 被引量:17

3尤显卿,宋雪峰,张成军,马建国,黄曼平.电冶稀土WC钢结硬质合金中碳化物特征的研究[J].材料热处理学报,2006,27(6):74-77. 被引量:9

4张焱,尤显卿,田四光,钟成山,丁峰.钢结硬质合金的发展现状[J].热处理,2008,23(1):12-15. 被引量:14

5王澈,钟涛兴,周美玲.WC钢结硬质合金再生研究[J].硬质合金,2001,18(3):146-149.

6王澈,钟涛兴,周美玲.钢结硬质合金预合金粉的研究[J].稀有金属与硬质合金,2002,30(2):7-10. 被引量:1

7尤显卿,黄曼平,郑玉春,程娟文.电冶熔铸碳化钨钢结硬质合金的微观组织研究[J].矿冶工程,2003,23(2):87-90. 被引量:8

1李云峰,石岩.WC对激光熔覆层组织及耐磨耐冲击性的影响[J].中国表面工程,2021,34(2):104-113. 被引量:7

2尤显卿,马建国,宋雪峰,任昊,黄曼平.电冶熔铸WC/钢复合材料中WC的溶解行为[J].中国有色金属学报,2005,15(9):1363-1368. 被引量:17

3钟正彬,魏晓伟.钢结硬质合金-铸钢镶铸的研究[J].热加工工艺,2005,34(10):15-17. 被引量:11

4张成军,尤显卿,宋雪峰,黄曼平,马建国.激光重熔对电冶钢结硬质合金表面显微组织的影响[J].硬质合金,2006,23(4):198-202. 被引量:4

5黄曼平,尤显卿,宋雪峰,张成军,马建国.电冶熔铸WC/钢复合材料组织及碳化物演变的研究[J].铸造技术,2007,28(8):1053-1058. 被引量:13

6黄曼平,尤显卿,马建国,黄世亮,张世军.激光重熔对电冶钢结硬质合金DGJW40组织影响的研究[J].材料热处理学报,2007,28(4):130-134. 被引量:1

7王智慧,杨爱弟,张田,贺定勇.真空熔覆WC颗粒增强复合涂层中WC溶解行为的研究[J].材料工程,2008,36(9):56-59. 被引量:9

8叶劲,尤显卿,黄曼平,马建国,刘宝.WC_P/钢基复合材料及复合轧辊的研究进展[J].稀有金属与硬质合金,2008,36(3):48-53. 被引量:7

9龚伟,李华,朱勇.淬火对(Ti,V)C钢结硬质合金组织及硬度的影响[J].热加工工艺,2009,38(6):136-140. 被引量:3

10龚伟,李华,要小鹏.(Ti,V)C钢结硬质合金的烧结行为、物相及组织结构[J].钢铁钒钛,2009,30(2):80-85. 被引量:2

1王澈,钟涛兴,周美玲.钢结硬质合金预合金粉的研究[J].稀有金属与硬质合金,2002,30(2):7-10. 被引量:1

2王澈,钟涛兴,周美玲.预合金粉制作钢结硬质合金组织的研究[J].稀有金属与硬质合金,2001,29(3):6-9. 被引量:1

3邱.碳化钨基硬质合金粉末[J].工具展望,2004(2):20-20.

4左洪松,栾道成,王正云,李亚军,秦琴.不同含量复式碳化物对细晶硬质合金性能的影响[J].中国钨业,2011,26(6):27-30. 被引量:6

5吴悦梅,易磊隽,王新玲,熊计.WC含量对Ti(C,N)基金属陶瓷显微组织的影响[J].钢铁钒钛,2016,37(6):56-60. 被引量:4

6陈雪松.影响复式碳化物(TiC-WC)固溶氧含量有关因素的研究[J].硬质合金,1999,16(3):159-161.

7王澈,钟涛兴,周美玲.WC钢结硬质合金再生研究[J].硬质合金,2001,18(3):146-149.

8何木光.炼钢污泥浆浓度对烧结的影响[J].矿业工程,2016,14(6):40-42. 被引量:1

9熊心志.武钢一、二烧车间熔剂准备系统的设计特点[J].烧结球团,1993,18(5):19-21.

10左中眉,栾道成,田瀚林,陈晓男.(W,Ti,Ta)C复式碳化物对WC-(6%~8%)Co超细硬质合金性能的影响[J].中国钨业,2013,28(5):36-40. 被引量:2

Basic Information:

DOI:

Chinese Library Classification Number:TF125.32[冶金工程—粉末冶金]

Citation Information:

Analysis is made of the structure of WC based steel bonded molten and annealed cemented carbides and study was made of the influence of different carbon addition on the structure,The results showed that WC is not present in the structure of molten steel bonded cemented carbide.Proper increase of carbon or WC content and annealing will help improve the improper structures and WC reduction.

quote

GB/T 7714-2015 [1] WANG Che, ZHONG Tao-xing, ZHOU Mei-ling. Investigation on Microstructure of Steel-bonded Molten Cemented Carbides[J]. Rare Metals and Cemented Carbides, 2001(1): 18-23.
MLA [1] WANG Che, et al., "Investigation on Microstructure of Steel-bonded Molten Cemented Carbides." Rare Metals and Cemented Carbides, no. 1, 2001, pp. 18-23.
APA [1] WANG Che, ZHONG Tao-xing, & ZHOU Mei-ling. (2001). Investigation on Microstructure of Steel-bonded Molten Cemented Carbides. Rare Metals and Cemented Carbides(1), 18-23.
IEEE [1] WANG Che, ZHONG Tao-xing, and ZHOU Mei-ling, "Investigation on Microstructure of Steel-bonded Molten Cemented Carbides," Rare Metals and Cemented Carbides, no. 1, pp. 18-23, 2001. keywords: {steel bonded cemented carbide;melting;C content;cemented carbide compound;annealing treatment.}