Tetracycline-Loaded Electrospun Poly(l-lactide-co-ε-caprolactone) Membranes for One-Step Periodontal Treatment AITranslate
Abstract AITranslate
In this research, a one-step periodontal membrane, with the required function and properties, has been designed as an alternative method of tissue regenerative treatments. Designed nanoporous prototypes from poly(l-lactide-co-ε-caprolactone) (PLCL, 70:30 mol %) were fabricated by electrospinning, denoted as S-PLCL. They were subsequently loaded with tetracycline (TC) in order to enhance periodontal regeneration and deliver an anti-inflammatory and antibiotic drug. It was found that TC loading did not have any significant effect on the fiber diameter but did increase hydrophilicity. With the increase in TC loading, the water vapor permeability (WVP) of the S-PLCL membrane decreased within the range of 31–56% when compared with neat S-PLCL membranes, while in the solvent-cast film (F-PLCL), no significant change in WVP was observed. Moreover, S-PLCL demonstrated a controllable slow release rate of TC. S-PLCL loaded with 1500 μg/mL of TC showed a release concentration of 30 ppm over a certain time period to promote greater levels of human oral fibroblast and human oral keratinocyte cell proliferation and plaque inhibition. In conclusion, a TC-loaded S-PLCL fibrous membrane has been designed and fabricated to provide the ideal conditions for cell proliferation and antibiotic activity during treatment, outperforming nonfibrous F-PLCL loaded with TC at the same concentration.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c01794
Chinese Library Classification Number:
Citation Information:
In this research, a one-step periodontal membrane, with the required function and properties, has been designed as an alternative method of tissue regenerative treatments. Designed nanoporous prototypes from poly(l-lactide-co-ε-caprolactone) (PLCL, 70:30 mol %) were fabricated by electrospinning, denoted as S-PLCL. They were subsequently loaded with tetracycline (TC) in order to enhance periodontal regeneration and deliver an anti-inflammatory and antibiotic drug. It was found that TC loading did not have any significant effect on the fiber diameter but did increase hydrophilicity. With the increase in TC loading, the water vapor permeability (WVP) of the S-PLCL membrane decreased within the range of 31–56% when compared with neat S-PLCL membranes, while in the solvent-cast film (F-PLCL), no significant change in WVP was observed. Moreover, S-PLCL demonstrated a controllable slow release rate of TC. S-PLCL loaded with 1500 μg/mL of TC showed a release concentration of 30 ppm over a certain time period to promote greater levels of human oral fibroblast and human oral keratinocyte cell proliferation and plaque inhibition. In conclusion, a TC-loaded S-PLCL fibrous membrane has been designed and fabricated to provide the ideal conditions for cell proliferation and antibiotic activity during treatment, outperforming nonfibrous F-PLCL loaded with TC at the same concentration.
quote
| GB/T 7714-2015 | [1] Thannaphat Jenvoraphot, Boontharika Thapsukhon, Donraporn Daranarong, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01794. |
| MLA | [1] Thannaphat Jenvoraphot, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01794. |
| APA | [1] Thannaphat Jenvoraphot, Boontharika Thapsukhon, Donraporn Daranarong, Robert Molloy, Chayarop Supanchart, Suttichai Krisanaprakornkit, Paul D. Topham, Brian Tighe, Anisa Mahomed, & Winita Punyodom. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01794 |
| IEEE | [1] Thannaphat Jenvoraphot, Boontharika Thapsukhon, Donraporn Daranarong, Robert Molloy, Chayarop Supanchart, Suttichai Krisanaprakornkit, Paul D. Topham, Brian Tighe, Anisa Mahomed, and Winita Punyodom, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01794. keywords: {poly(llactidecoεcaprolactone);biodegradable;tetracycline;electrospinning;controlled release;periodontitis treatment;Show More} |