daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Cross-linking Poly(caprolactone)–Polyamidoamine Linear Dendritic Block Copolymers for Theranostic Nanomedicine AITranslate

University; University; Southern Methodist University; Auburn University; University; University; The University of Southern Mississippi; University; The University of Southern Mississippi; University; Auburn University; Southern Methodist University; University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

This study represents a comparative analysis of the solution behavior and self-assembly pattern of two linear dendritic block copolymers (LDBCs) composed of a generation 3 polyamidoamine (PAMAM) dendron as the dendritic block and poly(caprolactone) (PCL) as the linear block, the latter of which is modified with pendant phenyl groups. Phenyl substituents were introduced to induce physical cross-linking in LDBC nanoparticles via π–π stacking. A synthetic strategy was developed to access phenyl substituted LDBCs through an ε-caprolactone monomer derivative followed by ring-opening polymerization to form a library of LDBCs with yields above 83%. Polymersome-like nanoparticles were observed in water with a 74.4 nm average diameter. Cross-linked LDBC nanoparticles demonstrated a 37.1% relative decrease in the critical aggregation concentration (CAC) and a 27.3–41.2% relative increase of hydrophobic loading efficiency relative to unsubstituted LDBCs. Nanoparticles loaded with a potential photothermal agent (phenyl indolizine-C5 (C5)) showed a photothermal efficiency of 49.4% with a heating temperature of 44.4 °C. These nanoparticles were efficiently loaded into HEK293 cells with cell viability above 87.5% at the highest concentration. Upon illumination with red light, nanoparticles loaded with photothermal agent were able to induce cell death in cancer cells. This work suggests that the phenyl substituted LDBCs form nanoparticles with enhanced stability and loading efficiencies compared to conventional nonphenylated systems and display a greater potential to be used as nanocarriers in theranostic nanomedicine.

KeyWords AITranslate

nanomedicine photothermal therapy NIR imaging theranostics selfassembly nanoparticles
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01131

Chinese Library Classification Number:

Citation Information:

This study represents a comparative analysis of the solution behavior and self-assembly pattern of two linear dendritic block copolymers (LDBCs) composed of a generation 3 polyamidoamine (PAMAM) dendron as the dendritic block and poly(caprolactone) (PCL) as the linear block, the latter of which is modified with pendant phenyl groups. Phenyl substituents were introduced to induce physical cross-linking in LDBC nanoparticles via π–π stacking. A synthetic strategy was developed to access phenyl substituted LDBCs through an ε-caprolactone monomer derivative followed by ring-opening polymerization to form a library of LDBCs with yields above 83%. Polymersome-like nanoparticles were observed in water with a 74.4 nm average diameter. Cross-linked LDBC nanoparticles demonstrated a 37.1% relative decrease in the critical aggregation concentration (CAC) and a 27.3–41.2% relative increase of hydrophobic loading efficiency relative to unsubstituted LDBCs. Nanoparticles loaded with a potential photothermal agent (phenyl indolizine-C5 (C5)) showed a photothermal efficiency of 49.4% with a heating temperature of 44.4 °C. These nanoparticles were efficiently loaded into HEK293 cells with cell viability above 87.5% at the highest concentration. Upon illumination with red light, nanoparticles loaded with photothermal agent were able to induce cell death in cancer cells. This work suggests that the phenyl substituted LDBCs form nanoparticles with enhanced stability and loading efficiencies compared to conventional nonphenylated systems and display a greater potential to be used as nanocarriers in theranostic nanomedicine.

quote

GB/T 7714-2015 [1] Indika Chandrasiri, Mahesh Loku Yaddehige, Bo Li, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01131.
MLA [1] Indika Chandrasiri, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01131.
APA [1] Indika Chandrasiri, Mahesh Loku Yaddehige, Bo Li, Yuzhe Sun, William E. Meador, Austin Dorris, Mohammad Farid Zia, Nathan I. Hammer, Alex Flynt, Jared H. Delcamp, Edward Davis, Alexander Lippert, & Davita L. Watkins. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01131
IEEE [1] Indika Chandrasiri, Mahesh Loku Yaddehige, Bo Li, Yuzhe Sun, William E. Meador, Austin Dorris, Mohammad Farid Zia, Nathan I. Hammer, Alex Flynt, Jared H. Delcamp, Edward Davis, Alexander Lippert, and Davita L. Watkins, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01131. keywords: {nanomedicine;photothermal therapy;NIR imaging;theranostics;selfassembly;nanoparticles}