Interdigitating Elastic Fibers with a Liquid Metal Core toward Ultrastretchable and Soft Capacitive Sensors: From 1D Fibers to 2D Electronics Interdigitating Elastic Fibers with a Liquid Metal Core toward Ultrastretchable and Soft Capacitive Sensors: From 1D Fibers to 2D Electronics AITranslate

Jeonbuk National University; Jeonbuk National University; Korea Institute of Science and Technology (KIST); Korea Institute of Science and Technology (KIST);Sustainable Materials Research Team, Research & Development Division; Jeonbuk National University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Ultrastretchable and elastic fibers with a liquid metal (EGaIn, eutectic alloy of gallium and indium) core were utilized to fabricate 2D capacitive sensors by arranging the fibers in an interdigitated structure. Once the fibers were prepared by simple roller coating, interdigitated structures were formed by plasma-activated chemical bonding of the fibers. EGaIn was injected into the core of the hollow elastic fibers, resulting in 2D capacitive sensors with dielectrics between the in-plane interdigitated electrodes. The liquid metal used in this work preserves the metallic conductivity upon strain because of the fluidic nature of the metal. Thus, the capacitance can be manipulated by the strain (upon mechanical deformation) of interdigitated fibers. The out-of-plane fringe electric field generated at the edges of the in-plane interdigitated liquid metal electrodes can be interfered with by adjacent objects or solvents surrounding the fibers due to various dielectric constants of the medium, resulting in a varying capacitance. This approach of fabricating 2D capacitive sensors from 1D fibers with a liquid metal core can be implemented in electronic textiles, wearable sensors, and soft robotics, owing to the fiber-form factor as well as the deformable electrical conductivity of the liquid metal wire.

KeyWords AITranslate

liquid metal ultrastretchable elastic fiber stretchable electronics wearable sensor human machine interfaceShow More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c01382

Chinese Library Classification Number:

Citation Information:

Ultrastretchable and elastic fibers with a liquid metal (EGaIn, eutectic alloy of gallium and indium) core were utilized to fabricate 2D capacitive sensors by arranging the fibers in an interdigitated structure. Once the fibers were prepared by simple roller coating, interdigitated structures were formed by plasma-activated chemical bonding of the fibers. EGaIn was injected into the core of the hollow elastic fibers, resulting in 2D capacitive sensors with dielectrics between the in-plane interdigitated electrodes. The liquid metal used in this work preserves the metallic conductivity upon strain because of the fluidic nature of the metal. Thus, the capacitance can be manipulated by the strain (upon mechanical deformation) of interdigitated fibers. The out-of-plane fringe electric field generated at the edges of the in-plane interdigitated liquid metal electrodes can be interfered with by adjacent objects or solvents surrounding the fibers due to various dielectric constants of the medium, resulting in a varying capacitance. This approach of fabricating 2D capacitive sensors from 1D fibers with a liquid metal core can be implemented in electronic textiles, wearable sensors, and soft robotics, owing to the fiber-form factor as well as the deformable electrical conductivity of the liquid metal wire.

quote

GB/T 7714-2015 [1] Sangmin Lee, Priyanuj Bhuyan, Kwak Jin Bae, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c01382.
MLA [1] Sangmin Lee, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c01382.
APA [1] Sangmin Lee, Priyanuj Bhuyan, Kwak Jin Bae, Jaesang Yu, Hongchan Jeon, & Sungjune Park. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c01382
IEEE [1] Sangmin Lee, Priyanuj Bhuyan, Kwak Jin Bae, Jaesang Yu, Hongchan Jeon, and Sungjune Park, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c01382. keywords: {liquid metal ultrastretchable elastic fiber stretchable electronics wearable sensor human machine interfaceShow More}