Crosslinking of Branched PIM-1 and PIM-Py Membranes for Recovery of Toluene from Dimethyl Sulfoxide by Pervaporation AITranslate
Abstract AITranslate
Branched forms of the archetypal polymer of intrinsic microporosity PIM-1 and the pyridinecarbonitrile-containing PIM-Py may be crosslinked under ambient conditions by palladium(II) acetate. Branched PIM-1 can arise in polymerizations of 5,5′,6,6′-tetrahydroxy-3,3,3′,3′-tetramethyl-1,1′-spirobisindane with tetrafluoroterephthalonitrile conducted at a high set temperature (160 °C) under conditions, such as high dilution, that lead to a lower-temperature profile over the course of the reaction. Membranes of PIM-1 and PIM-Py crosslinked with palladium acetate are sufficiently stable in organic solvents for use in the recovery of toluene from its mixture with dimethyl sulfoxide (DMSO) by pervaporation at 65 °C. With both PIM-1 and PIM-Py membranes, pervaporation gives high toluene/DMSO separation factors (around 10 with a 77 vol % toluene feed). Detailed analysis shows that the membranes themselves are slightly selective for DMSO and it is the high driving force for toluene evaporation that drives the separation.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.2c01600
Chinese Library Classification Number:
Citation Information:
Branched forms of the archetypal polymer of intrinsic microporosity PIM-1 and the pyridinecarbonitrile-containing PIM-Py may be crosslinked under ambient conditions by palladium(II) acetate. Branched PIM-1 can arise in polymerizations of 5,5′,6,6′-tetrahydroxy-3,3,3′,3′-tetramethyl-1,1′-spirobisindane with tetrafluoroterephthalonitrile conducted at a high set temperature (160 °C) under conditions, such as high dilution, that lead to a lower-temperature profile over the course of the reaction. Membranes of PIM-1 and PIM-Py crosslinked with palladium acetate are sufficiently stable in organic solvents for use in the recovery of toluene from its mixture with dimethyl sulfoxide (DMSO) by pervaporation at 65 °C. With both PIM-1 and PIM-Py membranes, pervaporation gives high toluene/DMSO separation factors (around 10 with a 77 vol % toluene feed). Detailed analysis shows that the membranes themselves are slightly selective for DMSO and it is the high driving force for toluene evaporation that drives the separation.
quote
| GB/T 7714-2015 | [1] Sulaiman Aloraini, Michael Mathias, Jessica Crone, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c01600. |
| MLA | [1] Sulaiman Aloraini, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c01600. |
| APA | [1] Sulaiman Aloraini, Michael Mathias, Jessica Crone, Kurtis Bryce, Ming Yu, Richard A. Kirk, Mohd Zamidi Ahmad, Edidiong D. Asuquo, Sandra RicoMartínez, Alexey V. Volkov, Andrew B. Foster, & Peter M. Budd. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c01600 |
| IEEE | [1] Sulaiman Aloraini, Michael Mathias, Jessica Crone, Kurtis Bryce, Ming Yu, Richard A. Kirk, Mohd Zamidi Ahmad, Edidiong D. Asuquo, Sandra RicoMartínez, Alexey V. Volkov, Andrew B. Foster, and Peter M. Budd, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c01600. keywords: {polymer of intrinsic microporosity;crosslinking;pervaporation;organic−organic separation;branched PIMs} |