Mechanism of the Zinc Dithiocarbamate-Activated Rubber Vulcanization Process: A Density Functional Theory Study AITranslate

Beijing University of Chemical Technology; Beijing University of Chemical Technology;BeijingYanshan Petrochemical High-Tech Co., Ltd. Sinopec Group; Hebei University; Beijing University of Chemical Technology; Beijing University of Chemical Technology; Beijing University of Chemical Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

To elucidate the mechanism of sulfur vulcanization of butadiene-styrene rubber by zinc dithiocarbamate (ZDMC), the density functional theory method was used to investigate the nature of the vulcanization induction and vulcanization periods of the rubber vulcanization process mediated by ZDMC. A mechanism for the sulfur pyrolysis by bimolecular ZDMC during the vulcanization induction period is proposed in which sulfur is inserted to produce active sulfurating agents. The calculated results indicate that the cross-link precursors of perthiols are generated in the reaction of active vulcanizing agents and single chains of rubber molecules and that ZDMC could promote the cross-linking of cross-link precursors during vulcanization to form the vulcanizate. This work established the mechanism of Zn(II)-activated sulfur vulcanization, which provided theoretical insights into the development of the rubber vulcanization accelerators.

KeyWords AITranslate

rubber ZDMCactivated vulcanization accelerator crosslinking agent DFT calculation
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00902

Chinese Library Classification Number:

Citation Information:

To elucidate the mechanism of sulfur vulcanization of butadiene-styrene rubber by zinc dithiocarbamate (ZDMC), the density functional theory method was used to investigate the nature of the vulcanization induction and vulcanization periods of the rubber vulcanization process mediated by ZDMC. A mechanism for the sulfur pyrolysis by bimolecular ZDMC during the vulcanization induction period is proposed in which sulfur is inserted to produce active sulfurating agents. The calculated results indicate that the cross-link precursors of perthiols are generated in the reaction of active vulcanizing agents and single chains of rubber molecules and that ZDMC could promote the cross-linking of cross-link precursors during vulcanization to form the vulcanizate. This work established the mechanism of Zn(II)-activated sulfur vulcanization, which provided theoretical insights into the development of the rubber vulcanization accelerators.

quote

GB/T 7714-2015 [1] Fuxing Shi, Xiaolin Li, Yinna Bai, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00902.
MLA [1] Fuxing Shi, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00902.
APA [1] Fuxing Shi, Xiaolin Li, Yinna Bai, Longfei Li, Min Pu, Li Liu, & Ming Lei. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00902
IEEE [1] Fuxing Shi, Xiaolin Li, Yinna Bai, Longfei Li, Min Pu, Li Liu, and Ming Lei, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00902. keywords: {rubber;ZDMCactivated;vulcanization accelerator;crosslinking agent;DFT calculation}