daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Depolymerizable Polyimines Triggered by Heat or Acid as Binders for Conductive Inks AITranslate

2500 Blvd de l’Université; 2500 Blvd de l’Université
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The ability to print electronic devices on soft substrates has the potential to revolutionize the world of consumable electronics. Electronic inks are typically constituted of an active nanomaterial dispersed in a solvent and stabilized by a surfactant which is necessary to impart colloidal stability. However, once the ink is applied, the surfactant presence in the final product is detrimental to the device performance. Here, we report the preparation of polyimines that can depolymerize and evaporate in the presence of light and heat. These polyimines were used for the formulation of Ag nanoparticle inks as well as for the dispersion of multiwalled carbon nanotubes (MWCNTs). In both cases, stable dispersions were obtained and were applied on a variety of substrates, leading to low-conductivity inks. However, the depolymerization and evaporation of the polyimine surfactant could be triggered by light and heat, then leading to a high-conductivity ink. By use of a laser engraver equipped with a CO2 laser, it was possible to spatially control the depolymerization of the MWCNT ink applied on a poly(ethylene terephthalate) film, while the nonexposed MWCNT ink was removed by simple solvent washing. Via this technique, it was possible to direct-write MWCNTs on a flexible substrate, thus demonstrating the potential of polyimines for the fabrication of electronic inks.

KeyWords AITranslate

polyimine depolymerization conductive ink carbon nanotubes dispersion
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00491

Chinese Library Classification Number:

Citation Information:

The ability to print electronic devices on soft substrates has the potential to revolutionize the world of consumable electronics. Electronic inks are typically constituted of an active nanomaterial dispersed in a solvent and stabilized by a surfactant which is necessary to impart colloidal stability. However, once the ink is applied, the surfactant presence in the final product is detrimental to the device performance. Here, we report the preparation of polyimines that can depolymerize and evaporate in the presence of light and heat. These polyimines were used for the formulation of Ag nanoparticle inks as well as for the dispersion of multiwalled carbon nanotubes (MWCNTs). In both cases, stable dispersions were obtained and were applied on a variety of substrates, leading to low-conductivity inks. However, the depolymerization and evaporation of the polyimine surfactant could be triggered by light and heat, then leading to a high-conductivity ink. By use of a laser engraver equipped with a CO2 laser, it was possible to spatially control the depolymerization of the MWCNT ink applied on a poly(ethylene terephthalate) film, while the nonexposed MWCNT ink was removed by simple solvent washing. Via this technique, it was possible to direct-write MWCNTs on a flexible substrate, thus demonstrating the potential of polyimines for the fabrication of electronic inks.

quote

GB/T 7714-2015 [1] Barbara Martin, Jerome P. Claverie. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00491.
MLA [1] Barbara Martin, and Jerome P. Claverie. ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00491.
APA [1] Barbara Martin, & Jerome P. Claverie. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00491
IEEE [1] Barbara Martin and Jerome P. Claverie, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00491. keywords: {polyimine;depolymerization;conductive ink;carbon nanotubes;dispersion}