Additive Manufactured Scaffolds for Bone Tissue Engineering: Physical Characterization of Thermoplastic Composites with Functional Fillers AITranslate

Maastricht University;TECNALIA, Basque Research and Technology Alliance (BRTA); Maastricht University;TECNALIA, Basque Research and Technology Alliance (BRTA); Maastricht University;Biobased Materials;University of Naples Federico II;University of Naples Federico II;University of Naples Federico II;Prolabin & Tefarm S.r.l., Perugia 06134;Nadir S.r.l.;Abalonyx AS, Oslo 0373;TECNALIA, Basque Research and Technology Alliance (BRTA);TECNALIA, Basque Research and Technology Alliance (BRTA);Centro de Fisica de Materiales (CSIC; Padova University;University of Naples Federico II; Maastricht University; Maastricht University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Thermoplastic polymer–filler composites are excellent materials for bone tissue engineering (TE) scaffolds, combining the functionality of fillers with suitable load-bearing ability, biodegradability, and additive manufacturing (AM) compatibility of the polymer. Two key determinants of their utility are their rheological behavior in the molten state, determining AM processability and their mechanical load-bearing properties. We report here the characterization of both these physical properties for four bone TE relevant composite formulations with poly(ethylene oxide terephthalate)/poly(butylene terephthalate (PEOT/PBT) as a base polymer, which is often used to fabricate TE scaffolds. The fillers used were reduced graphene oxide (rGO), hydroxyapatite (HA), gentamicin intercalated in zirconium phosphate (ZrP-GTM) and ciprofloxacin intercalated in MgAl layered double hydroxide (MgAl-CFX). The rheological assessment showed that generally the viscous behavior dominated the elastic behavior (G″ > G′) for the studied composites, at empirically determined extrusion temperatures. Coupled rheological–thermal characterization of ZrP-GTM and HA composites showed that the fillers increased the solidification temperatures of the polymer melts during cooling. Both these findings have implications for the required extrusion temperatures and bonding between layers. Mechanical tests showed that the fillers generally not only made the polymer stiffer but more brittle in proportion to the filler fractions. Furthermore, the elastic moduli of scaffolds did not directly correlate with the corresponding bulk material properties, implying composite-specific AM processing effects on the mechanical properties. Finally, we show computational models to predict multimaterial scaffold elastic moduli using measured single material scaffold and bulk moduli. The reported characterizations are essential for assessing the AM processability and ultimately the suitability of the manufactured scaffolds for the envisioned bone regeneration application.

KeyWords AITranslate

composites fillers rheology mechanical properties modeling additive manufacturing
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00363

Chinese Library Classification Number:

Citation Information:

Thermoplastic polymer–filler composites are excellent materials for bone tissue engineering (TE) scaffolds, combining the functionality of fillers with suitable load-bearing ability, biodegradability, and additive manufacturing (AM) compatibility of the polymer. Two key determinants of their utility are their rheological behavior in the molten state, determining AM processability and their mechanical load-bearing properties. We report here the characterization of both these physical properties for four bone TE relevant composite formulations with poly(ethylene oxide terephthalate)/poly(butylene terephthalate (PEOT/PBT) as a base polymer, which is often used to fabricate TE scaffolds. The fillers used were reduced graphene oxide (rGO), hydroxyapatite (HA), gentamicin intercalated in zirconium phosphate (ZrP-GTM) and ciprofloxacin intercalated in MgAl layered double hydroxide (MgAl-CFX). The rheological assessment showed that generally the viscous behavior dominated the elastic behavior (G″ > G′) for the studied composites, at empirically determined extrusion temperatures. Coupled rheological–thermal characterization of ZrP-GTM and HA composites showed that the fillers increased the solidification temperatures of the polymer melts during cooling. Both these findings have implications for the required extrusion temperatures and bonding between layers. Mechanical tests showed that the fillers generally not only made the polymer stiffer but more brittle in proportion to the filler fractions. Furthermore, the elastic moduli of scaffolds did not directly correlate with the corresponding bulk material properties, implying composite-specific AM processing effects on the mechanical properties. Finally, we show computational models to predict multimaterial scaffold elastic moduli using measured single material scaffold and bulk moduli. The reported characterizations are essential for assessing the AM processability and ultimately the suitability of the manufactured scaffolds for the envisioned bone regeneration application.

quote

GB/T 7714-2015 [1] Ravi Sinha, Alberto Sanchez, Maria CamaraTorres, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00363.
MLA [1] Ravi Sinha, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00363.
APA [1] Ravi Sinha, Alberto Sanchez, Maria CamaraTorres, Iñigo Calderon UriszarAldaca, Andrea Roberto Calore, Jules Harings, Ambra Gambardella, Lucia Ciccarelli, Veronica Vanzanella, Michele Sisani, Marco Scatto, Rune Wendelbo, Sergio Perez, Sara Villanueva, Amaia Matanza, Alessandro Patelli, Nino Grizzuti, Carlos Mota, & Lorenzo Moroni. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00363
IEEE [1] Ravi Sinha, Alberto Sanchez, Maria CamaraTorres, Iñigo Calderon UriszarAldaca, Andrea Roberto Calore, Jules Harings, Ambra Gambardella, Lucia Ciccarelli, Veronica Vanzanella, Michele Sisani, Marco Scatto, Rune Wendelbo, Sergio Perez, Sara Villanueva, Amaia Matanza, Alessandro Patelli, Nino Grizzuti, Carlos Mota, and Lorenzo Moroni, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00363. keywords: {composites;fillers;rheology;mechanical properties;modeling;additive manufacturing}