Stretchable Nanostructures as Optomechanical Strain Sensors for Ophthalmic Applications AITranslate

University of Birmingham; University of Birmingham; Imperial College London; University of Sydney; University of Birmingham; Imperial College London
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The intraocular pressure (IOP) is a physiological parameter that plays a crucial role in preventing, diagnosing, and treating ocular diseases. For example, lowering the IOP is the primary focus of glaucoma management. However, IOP is a widely varying parameter, and one-off measurements are prompt to errors. Developing portable solutions for continuous monitoring the IOP is a critical goal in ophthalmology. Here, stretchable nanostructures were developed as strain-tunable diffraction gratings and integrated into a contact lens. They exhibited a limit of detection (LOD) <2 mmHg and a linear response in the range of interest (15–35 mmHg). Nanopatterns were characterized under monochromatic laser sources and further integrated into a soft contact lens. A smartphone readout method based on preferentially reflected colors was proposed to pave the way toward smartphone-based ocular health monitoring.

KeyWords AITranslate

nanopillars diffraction gratings contact lenses intraocular pressure (IOP) glaucoma
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00703

Chinese Library Classification Number:

Citation Information:

The intraocular pressure (IOP) is a physiological parameter that plays a crucial role in preventing, diagnosing, and treating ocular diseases. For example, lowering the IOP is the primary focus of glaucoma management. However, IOP is a widely varying parameter, and one-off measurements are prompt to errors. Developing portable solutions for continuous monitoring the IOP is a critical goal in ophthalmology. Here, stretchable nanostructures were developed as strain-tunable diffraction gratings and integrated into a contact lens. They exhibited a limit of detection (LOD) <2 mmHg and a linear response in the range of interest (15–35 mmHg). Nanopatterns were characterized under monochromatic laser sources and further integrated into a soft contact lens. A smartphone readout method based on preferentially reflected colors was proposed to pave the way toward smartphone-based ocular health monitoring.

quote

GB/T 7714-2015 [1] Rosalia Moreddu, Nasim Mahmoodi, Panagiotis Kassanos, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00703.
MLA [1] Rosalia Moreddu, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00703.
APA [1] Rosalia Moreddu, Nasim Mahmoodi, Panagiotis Kassanos, Daniele Vigolo, Paula M. Mendes, & Ali K. Yetisen. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00703
IEEE [1] Rosalia Moreddu, Nasim Mahmoodi, Panagiotis Kassanos, Daniele Vigolo, Paula M. Mendes, and Ali K. Yetisen, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00703. keywords: {nanopillars;diffraction gratings;contact lenses;intraocular pressure (IOP);glaucoma}