daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Drop-on-Demand Electrohydrodynamic Jet Printing of Microlens Array on Flexible Substrates AITranslate

Sungkyunkwan University; Sungkyunkwan University; Sungkyunkwan University; Sungkyunkwan University; Gyeongsang National University; Sungkyunkwan University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The inkjet-printing technique is regarded as an efficient method to fabricate microlens arrays used in digital cameras, medical endoscopes, displays, optical communication, and light source devices. The diameter, height, and aspect ratio of the microlens are the major contributors to these optical properties. Hence, the optical characteristics of the microlens array can vary with the type of inkjet-printing method. In this study, by employing electrohydrodynamic (EHD) jet printing with the drop-on-demand strategy, we fabricated microlenses and microlens arrays using a UV-curable photopolymer liquid on flexible poly(3,4-ethylenedioxythiophene):polystyrenesulfonate-coated poly(ethylene terephthalate). By controlling the number of printing drops, which is regarded as an efficient approach to control the dimension of the microlens, lenses with diameters of 11.9 ± 0.2 and 24.4 ± 0.5 μm and aspect ratio ranging from 0.22 to 0.33 were constructed. It was found that the focal length (15.44–26.79 μm), numerical aperture (0.39–0.46), and f-number (1.3–1.1) varied with the number of printing drops. The results demonstrate that the EHD-printed microlenses have a much shorter focal length, higher numerical aperture, and smaller f-number than the previously reported printed lenses. Hence, the EHD-printed microlens can be utilized to produce wide-angle-of-view applications and capture accurate images with insufficient light intensity. In addition, the proposed EHD-printing method may provide a cost-effective and simple route for manufacturing microlens arrays.

KeyWords AITranslate

electrohydrodynamic (EHD) jet printing microlens microlens arrays (MLAs) dropondemand (DoD) UVcurable photopolymer ink
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00054

Chinese Library Classification Number:

Citation Information:

The inkjet-printing technique is regarded as an efficient method to fabricate microlens arrays used in digital cameras, medical endoscopes, displays, optical communication, and light source devices. The diameter, height, and aspect ratio of the microlens are the major contributors to these optical properties. Hence, the optical characteristics of the microlens array can vary with the type of inkjet-printing method. In this study, by employing electrohydrodynamic (EHD) jet printing with the drop-on-demand strategy, we fabricated microlenses and microlens arrays using a UV-curable photopolymer liquid on flexible poly(3,4-ethylenedioxythiophene):polystyrenesulfonate-coated poly(ethylene terephthalate). By controlling the number of printing drops, which is regarded as an efficient approach to control the dimension of the microlens, lenses with diameters of 11.9 ± 0.2 and 24.4 ± 0.5 μm and aspect ratio ranging from 0.22 to 0.33 were constructed. It was found that the focal length (15.44–26.79 μm), numerical aperture (0.39–0.46), and f-number (1.3–1.1) varied with the number of printing drops. The results demonstrate that the EHD-printed microlenses have a much shorter focal length, higher numerical aperture, and smaller f-number than the previously reported printed lenses. Hence, the EHD-printed microlens can be utilized to produce wide-angle-of-view applications and capture accurate images with insufficient light intensity. In addition, the proposed EHD-printing method may provide a cost-effective and simple route for manufacturing microlens arrays.

quote

GB/T 7714-2015 [1] Busi Im, Fariza Dian Prasetyo, Hadi Teguh Yudistira, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00054.
MLA [1] Busi Im, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00054.
APA [1] Busi Im, Fariza Dian Prasetyo, Hadi Teguh Yudistira, Shaheer Mohiuddin Khalil, DaeHyun Cho, & Doyoung Byun. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00054
IEEE [1] Busi Im, Fariza Dian Prasetyo, Hadi Teguh Yudistira, Shaheer Mohiuddin Khalil, DaeHyun Cho, and Doyoung Byun, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00054. keywords: {electrohydrodynamic (EHD) jet printing;microlens;microlens arrays (MLAs);dropondemand (DoD);UVcurable photopolymer ink}