Porous Liquids as Electrolyte: A Case Study of Li+ and Mg2+ Ion Transport in Crown Ether-Based Type-II Porous Liquids AITranslate

Pacific Northwest National Laboratory; Pacific Northwest National Laboratory; Pacific Northwest National Laboratory; Pacific Northwest National Laboratory; Pacific Northwest National Laboratory; Pacific Northwest National Laboratory; Pacific Northwest National Laboratory; Pacific Northwest National Laboratory; Pacific Northwest National Laboratory; Pacific Northwest National Laboratory; Pacific Northwest National Laboratory
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

We demonstrated an enhanced ion transport properties of type-II porous liquid-based electrolyte in which crown ether provides internal porosity and are capable of coordinating and transporting Li+ and Mg2+ ions. We investigated the solvation structure and transport properties of the porous liquid electrolytes with different functional groups and cavity sizes. Among the electrolytes studied, the 12-crown-4 (12C4)-based porous liquid electrolyte exhibited the most enhanced ionic conductivity due to size match between the crown ether cavity and the Li+ ion. Nuclear magnetic resonance and Fourier transform infrared analyses revealed that addition of crown ethers reduces the Li+ ion–solvent interaction, resulting in the formation of Li-crown ether complexes. Molecular simulations complement such observations by describing the detailed solvation environment at molecular scale, including complexation between Li+ and Mg2+ ions and 12C4. The strategy described here using crown ether-based porous liquids should be applicable to design versatile electrolytes for various metal-ion batteries.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.2c00956

Chinese Library Classification Number:

Citation Information:

We demonstrated an enhanced ion transport properties of type-II porous liquid-based electrolyte in which crown ether provides internal porosity and are capable of coordinating and transporting Li+ and Mg2+ ions. We investigated the solvation structure and transport properties of the porous liquid electrolytes with different functional groups and cavity sizes. Among the electrolytes studied, the 12-crown-4 (12C4)-based porous liquid electrolyte exhibited the most enhanced ionic conductivity due to size match between the crown ether cavity and the Li+ ion. Nuclear magnetic resonance and Fourier transform infrared analyses revealed that addition of crown ethers reduces the Li+ ion–solvent interaction, resulting in the formation of Li-crown ether complexes. Molecular simulations complement such observations by describing the detailed solvation environment at molecular scale, including complexation between Li+ and Mg2+ ions and 12C4. The strategy described here using crown ether-based porous liquids should be applicable to design versatile electrolytes for various metal-ion batteries.

quote

GB/T 7714-2015 [1] Sun Hae Ra Shin, HyungSeok Lim, Kee Sung Han, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.2c00956.
MLA [1] Sun Hae Ra Shin, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.2c00956.
APA [1] Sun Hae Ra Shin, HyungSeok Lim, Kee Sung Han, Alexander J. Robinson, Aaron Hollas, Bhuvaneswari M. Sivakumar, Samantha I. Johnson, Jaehun Chun, Wei Wang, Vijayakumar Murugesan, & Praveen K. Thallapally. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.2c00956
IEEE [1] Sun Hae Ra Shin, HyungSeok Lim, Kee Sung Han, Alexander J. Robinson, Aaron Hollas, Bhuvaneswari M. Sivakumar, Samantha I. Johnson, Jaehun Chun, Wei Wang, Vijayakumar Murugesan, and Praveen K. Thallapally, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.2c00956.