Calculation of Secondary Phase Content in Hypoeutectic and Hypereutectic Alloys AITranslate

Changsha Industrial Higher Specialty School
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A simple calculation method for relative contents of secondary phase in hy poeutectic dissolubility solution and hypereutectic alloys of limited solid solution deduced in this paper it is of great importance for theoretical study on secondary phase

KeyWords AITranslate

hypoeutectic and hypereutectic alloys secondary phase calculation

1刘沙.低铼钼合金加工性能的研究[J].稀有金属与硬质合金,1998,26(1):33-36. 被引量:1

1辛甜,李延超,林小辉,常恬,高选乔,梁静.不同铼含量对钼铼合金性能影响研究概述[J].中国钼业,2022,46(6):1-8.

1曹京霞,黄旭,李臻熙.TA15钛合金的高周疲劳性能和断裂特征[J].材料工程,2004,32(3):28-30. 被引量:11

2孙晶,郭全英,毛萍莉,刘正.Mg-Al合金非平衡凝固共晶组织及形成机理[J].沈阳工业大学学报,2013,35(6):635-640. 被引量:2

3吴启权.齿轮加工最终进刀量的简便计算[J].机械工人:冷加工,1990(7):29-30.

4邹军涛,雷春娟,洪波,杨晓红.熔体保温时间对含硅蒙乃尔合金组织与硬度的影响[J].热加工工艺,2013,42(15):22-25.

5王哲,王新南,祝力伟,朱知寿.TB17钛合金等温时效析出行为[J].航空材料学报,2016,36(5):1-6. 被引量:15

6范翰,齐炜,王红武,庞洪.热处理工艺对TB5钛合金组织和性能的影响[J].中国钛业,2013(4):32-35.

7庞洪,齐炜,张永强,黄杰,王红武.热处理制度对90mm TC4 ELI宽幅厚板组织及性能的影响[J].中国钛业,2016(1):20-23.

8孙晶,厉虹,郭全英,毛萍莉,刘正.钙对Mg-8%Al镁合金组织及性能的影响[J].沈阳工业大学学报,2011,33(2):125-128. 被引量:3

9靳立坤,李晓延,贺定勇,蒋建敏,杨东霞,聂祚仁.含铒铝合金TIG焊接头组织与性能[J].焊接学报,2011,32(8):85-88. 被引量:3

10陈炳光.铝合金车轮挤压铸造余热淬火工艺理论及实践[J].特种铸造及有色合金,2001(S1):122-122. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TG113.12[金属学及工艺—物理冶金]

Citation Information:

A simple calculation method for relative contents of secondary phase in hy poeutectic dissolubility solution and hypereutectic alloys of limited solid solution deduced in this paper it is of great importance for theoretical study on secondary phase

quote

GB/T 7714-2015 [1] LIU Sha. Calculation of Secondary Phase Content in Hypoeutectic and Hypereutectic Alloys[J]. Rare Metals and Cemented Carbides, 1997(3): 52-53.
MLA [1] LIU Sha. "Calculation of Secondary Phase Content in Hypoeutectic and Hypereutectic Alloys." Rare Metals and Cemented Carbides, no. 3, 1997, pp. 52-53.
APA [1] LIU Sha. (1997). Calculation of Secondary Phase Content in Hypoeutectic and Hypereutectic Alloys. Rare Metals and Cemented Carbides(3), 52-53.
IEEE [1] LIU Sha, "Calculation of Secondary Phase Content in Hypoeutectic and Hypereutectic Alloys," Rare Metals and Cemented Carbides, no. 3, pp. 52-53, 1997. keywords: {hypoeutectic and hypereutectic alloys,secondary phase,calculation}