daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Adhesive Gel System Growable by Reversible Addition–Fragmentation Chain Transfer (RAFT) Polymerization AITranslate

Utsunomiya University; Utsunomiya University; Utsunomiya University; Utsunomiya University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Gel materials are materials with high elasticity that deform when stressed and then return to their original shapes once the stress is removed. Gel materials are expected to be used in artificial living tissues, soft robotics, sensors, and so on. On the other hand, humans grow and change their bodies and characteristics over time. In this research, we developed an adhesive gel system that can grow and change its characteristics like our humans after adhesion through reversible addition–fragmentation chain transfer (RAFT) polymerization, a class of living radical polymerization. The adhesive joint grown by RAFT polymerization had higher adhesive strength than the non-RAFT-polymerized adhesive joint and a function, i.e., thermal responsiveness of adhesive strength. The environment around us changes over time. These growable adhesive gel systems should enable us to use gel materials for a long time while adapting their structures and characteristics to environmental changes.

KeyWords AITranslate

adhesive system reversible addition−fragmentation chain transfer polymerization living radical polymerization gel soft material
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01913

Chinese Library Classification Number:

Citation Information:

Gel materials are materials with high elasticity that deform when stressed and then return to their original shapes once the stress is removed. Gel materials are expected to be used in artificial living tissues, soft robotics, sensors, and so on. On the other hand, humans grow and change their bodies and characteristics over time. In this research, we developed an adhesive gel system that can grow and change its characteristics like our humans after adhesion through reversible addition–fragmentation chain transfer (RAFT) polymerization, a class of living radical polymerization. The adhesive joint grown by RAFT polymerization had higher adhesive strength than the non-RAFT-polymerized adhesive joint and a function, i.e., thermal responsiveness of adhesive strength. The environment around us changes over time. These growable adhesive gel systems should enable us to use gel materials for a long time while adapting their structures and characteristics to environmental changes.

quote

GB/T 7714-2015 [1] Yuma Ueno, Hayato Nakazaki, Hina Onozaki, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c01913.
MLA [1] Yuma Ueno, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c01913.
APA [1] Yuma Ueno, Hayato Nakazaki, Hina Onozaki, & Shingo Tamesue. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c01913
IEEE [1] Yuma Ueno, Hayato Nakazaki, Hina Onozaki, and Shingo Tamesue, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c01913. keywords: {adhesive system;reversible addition−fragmentation chain transfer polymerization;living radical polymerization;gel;soft material}