The Latest Development of LiNi0.5Mn1.5O_4 Spinel Material AITranslate
Abstract AITranslate
The crystal structure and main preparation methods of LiNi0.5Mn1.5O4 spinel material are introduced.The methods to improve the charge and discharge rate and electrochemical performance of the material are reviewed including nano-sized synthesis,elemental doping,surface modification and so on.The future application of the material in the future advanced lithium ion battery is also pointed out.
KeyWords AITranslate
1范未峰,瞿美臻,彭工厂,于作龙.5V正极材料LiNi0.5Mn1.5O4的自蔓延燃烧合成及性能[J].无机化学学报,2009,25(1):124-128. 被引量:14
1王海龙.高压LiNi_(0.5)Mn_(1.5)O_4的机遇与挑战[J].广州化工,2013,41(19):30-31.
2谢玉虎,许鹏,杨续来,谢佳.高电压尖晶石镍锰酸锂材料全电池研究进展[J].电源技术,2014,38(3):551-552. 被引量:9
1谢佳,彭文,杨续来.尖晶石镍锰酸锂全电池常温循环寿命分析[J].储能科学与技术,2014,3(6):624-628. 被引量:2
2任春燕,叶学海,张春丽,夏继平,张晓波.高电压正极与电解液添加剂相容性研究[J].无机盐工业,2017,49(5):45-47. 被引量:2
3宫璐,曹利娜,张金龙.流变仪在锂离子电池中的应用[J].电源技术,2017,41(5):821-823. 被引量:1
4王玮.动力电池正极材料锰酸锂的改性及发展前景[J].电源技术,2017,41(9):1383-1385. 被引量:3
5武海燕,王嫣.基于多事件同步软件锰酸锂电池锂离子筛研究[J].电源技术,2017,41(8):1124-1126.
6罗军,田刚领,张柳丽,李娟,牛哲荟.钛酸锂体系锂离子电池综述[J].电源技术,2019,43(4):693-695. 被引量:13
7董海斌,尹国瑞,安普春,羡学磊,伊程毅.钛酸锂电池模组热失控扩展抑制技术研究[J].消防科学与技术,2021,40(6):779-782. 被引量:2
8董海斌,羡学磊,马建琴,伊程毅.锰酸锂电池热失控特性研究[J].消防科学与技术,2022,41(1):21-25.
9王春飞,袁桂霞,李华成,钟晴,黄瑞鸿.高电压镍锰酸锂LiNi_(0.5)Mn_(1.5)O_4制备实验研究[J].中国锰业,2017,35(S1):41-46. 被引量:1
1杜荣斌.尖晶石材料LiMn_2O_4的研究现状及展望[J].化工新型材料,2006,34(2):1-4. 被引量:4
2宰学荣.锂离子电池正极材料锂锰氧化物的研究进展[J].材料开发与应用,2002,17(2):39-42. 被引量:5
3蔡砚,王要武,何向明,姜长印,应皆荣,万春荣.尖晶石LiMn_2O_4容量衰减原因及对策[J].功能材料,2004,35(1):21-24. 被引量:23
4张永哲,武丽慧,刘彦平,谢二庆,闫德,陈江涛.Preparation of ZnO Nanospheres and Their Applications in Dye-Sensitized Solar Cells[J].中国物理快报:英文版,2009,26(3):283-286. 被引量:2
5胡晓宏,杨汉西,艾新平,李升宪,洪昕林.LiMn_2O_4正极在高温下性能衰退现象的研究[J].电化学,1999,5(2):224-230. 被引量:37
6于先进,邱竹贤,于亚鑫.铁锌、铁镍尖晶石材料的高温导电性[J].中国陶瓷,1998,34(1):14-15. 被引量:6
7詹晖,周运鸿.用新型的半固相方法合成掺钴尖晶石材料LiCo_xMn_(2-x)O_4及其性能研究[J].化学学报,2002,60(5):775-783. 被引量:1
8陈梅.日本开发出高输出能力的锂离子电池材料[J].电源技术,2010(12):1220-1222.
9冯传启,王世银,马军.Li4Ti5O12合成及电化学性质研究[J].功能材料,2007,38(A04):1431-1433.
10杨文柱,王珲,郑春满.LiMn_2O_4/LiNi_(0.8)Co_(0.15)Al_(0.05)O_2混合正极材料性能研究[J].广州化工,2016,44(15):51-54. 被引量:3
Basic Information:
DOI:
Chinese Library Classification Number:TM912.2[电气工程—电力电子与电力传动]
Citation Information:
The crystal structure and main preparation methods of LiNi0.5Mn1.5O4 spinel material are introduced.The methods to improve the charge and discharge rate and electrochemical performance of the material are reviewed including nano-sized synthesis,elemental doping,surface modification and so on.The future application of the material in the future advanced lithium ion battery is also pointed out.
quote
| GB/T 7714-2015 | [1] GAO Ya-jie, LIU Guo-qiang, ZHENG Jian-jie, et al. The Latest Development of LiNi0.5Mn1.5O_4 Spinel Material[J]. Rare Metals and Cemented Carbides, 2012(2): 19-23. |
| MLA | [1] GAO Ya-jie, et al., "The Latest Development of LiNi0.5Mn1.5O_4 Spinel Material." Rare Metals and Cemented Carbides, no. 2, 2012, pp. 19-23. |
| APA | [1] GAO Ya-jie, LIU Guo-qiang, ZHENG Jian-jie, & CEN Peng. (2012). The Latest Development of LiNi0.5Mn1.5O_4 Spinel Material. Rare Metals and Cemented Carbides(2), 19-23. |
| IEEE | [1] GAO Ya-jie, LIU Guo-qiang, ZHENG Jian-jie, and CEN Peng, "The Latest Development of LiNi0.5Mn1.5O_4 Spinel Material," Rare Metals and Cemented Carbides, no. 2, pp. 19-23, 2012. keywords: {lithium ion battery;cathode material;LiNi0.5Mn1.5O4;crystal structure;preparation methods;electrochemical performance} |