Design of Elastomer-Based Piezoresistive Sensors: Materials, Structural Aspects, and Prospects Design of Elastomer-Based Piezoresistive Sensors: Materials, Structural Aspects, and Prospects AITranslate

Jeonbuk National University;Metrology and Sensing Group, Samsung Electro-Mechanics Co.; Jeonbuk National University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Elastomer-based piezoresistive sensors are an impactful and promising means of monitoring biological motion, tracking biosignals, and measuring the mechanical collision of physical stimuli in robots or machines. Piezoresistive behavior is generally realized when conductivity is imparted to elastomers, which results in resistivity changes by an external force that induces elastic deformations. Piezoresistive behavior of an elastomer can be achieved by mixing or coating the elastomer with a conductive material, thereby forming a composite structure. In this review, the conductive and elastic components that may determine the performance of a sensor are introduced. Conductive materials are classified into metal fillers, carbon allotropes, and hybrid materials, while elastic structures are classified into nonperiodic/periodic, hierarchical, and textile-based formations. Then, this comprehensive review focuses on textile-based structures for flexible applications, emerging challenges, potential strategies, and finally, the proposed hybrid mechanisms.

KeyWords AITranslate

Piezoresistive sensor Elastomer Textile sensor Pressure/Strain sensor Microstructure
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c00039

Chinese Library Classification Number:

Citation Information:

Elastomer-based piezoresistive sensors are an impactful and promising means of monitoring biological motion, tracking biosignals, and measuring the mechanical collision of physical stimuli in robots or machines. Piezoresistive behavior is generally realized when conductivity is imparted to elastomers, which results in resistivity changes by an external force that induces elastic deformations. Piezoresistive behavior of an elastomer can be achieved by mixing or coating the elastomer with a conductive material, thereby forming a composite structure. In this review, the conductive and elastic components that may determine the performance of a sensor are introduced. Conductive materials are classified into metal fillers, carbon allotropes, and hybrid materials, while elastic structures are classified into nonperiodic/periodic, hierarchical, and textile-based formations. Then, this comprehensive review focuses on textile-based structures for flexible applications, emerging challenges, potential strategies, and finally, the proposed hybrid mechanisms.

quote

GB/T 7714-2015 [1] Youngwoo Kwak, Minkyu Choi, Changwoo Nam. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00039.
MLA [1] Youngwoo Kwak, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00039.
APA [1] Youngwoo Kwak, Minkyu Choi, & Changwoo Nam. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00039
IEEE [1] Youngwoo Kwak, Minkyu Choi, and Changwoo Nam, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00039. keywords: {Piezoresistive sensor Elastomer Textile sensor Pressure/Strain sensor Microstructure}