Enhancing Planar Perovskite Solar Cell Performance by SnO2 Interface Treatment Using Urea as an Additive: A Comparative Study of Simple, Low-Temperature Approaches Enhancing Planar Perovskite Solar Cell Performance by SnO2 Interface Treatment Using Urea as an Additive: A Comparative Study of Simple, Low-Temperature Approaches AITranslate

University of Tehran; Sharif University of Technology; University of Tehran; Sharif University of Technology; University of Tehran; University of Tehran; Sharif University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

For perovskite solar cells (PSCs), SnO2 is considered to be the most promising electron transport layer (ETL) material. Further, PSC performance enhancement is made possible through interface amendments, which were reported by several functional groups. Herein, successful n-type urea treatment of SnO2 is demonstrated by simple, low-temperature approaches of solution and spin-coating preparation. Considering the urea spin-coating and solution processes, the conductivity and electron transport of urea-doped SnO2 films have been dominantly improved, leading to enhanced PSC characteristics. Surface spin-coating is a more efficient method to add urea to SnO2 in comparison with precursor doping. On comparison, the PSCs with the surface spin-coated urea for SnO2 ETL offer the best power conversion efficiency (PCE) of 16.50%. However, under the same circumstances, the PSC made with the pure SnO2 ETL offers a PCE of 14.04%. The outcomes show a technique for improving the characteristics of PSCs. In the final part, to assess the impact of interfacial treatment on the performance of planar perovskite solar cells (PSCs), planar devices were simulated using Solar Cell Capacitance Simulator (SCAPS) software. The simulation incorporated crucial parameters from experimental analysis and reliable sources, ensuring reliability in the modeling process.

KeyWords AITranslate

planar perovskite solar cell ETL Urea−SnO2 SCAPS interface
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c00970

Chinese Library Classification Number:

Citation Information:

For perovskite solar cells (PSCs), SnO2 is considered to be the most promising electron transport layer (ETL) material. Further, PSC performance enhancement is made possible through interface amendments, which were reported by several functional groups. Herein, successful n-type urea treatment of SnO2 is demonstrated by simple, low-temperature approaches of solution and spin-coating preparation. Considering the urea spin-coating and solution processes, the conductivity and electron transport of urea-doped SnO2 films have been dominantly improved, leading to enhanced PSC characteristics. Surface spin-coating is a more efficient method to add urea to SnO2 in comparison with precursor doping. On comparison, the PSCs with the surface spin-coated urea for SnO2 ETL offer the best power conversion efficiency (PCE) of 16.50%. However, under the same circumstances, the PSC made with the pure SnO2 ETL offers a PCE of 14.04%. The outcomes show a technique for improving the characteristics of PSCs. In the final part, to assess the impact of interfacial treatment on the performance of planar perovskite solar cells (PSCs), planar devices were simulated using Solar Cell Capacitance Simulator (SCAPS) software. The simulation incorporated crucial parameters from experimental analysis and reliable sources, ensuring reliability in the modeling process.

quote

GB/T 7714-2015 [1] Razieh Teimouri, Razieh Keshtmand, Sajad Mehrvarz, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00970.
MLA [1] Razieh Teimouri, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00970.
APA [1] Razieh Teimouri, Razieh Keshtmand, Sajad Mehrvarz, Fatemeh Ghasemi, Ali Mahjoory, Mohammadreza Kolahdouz, & Nima Taghavinia. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00970
IEEE [1] Razieh Teimouri, Razieh Keshtmand, Sajad Mehrvarz, Fatemeh Ghasemi, Ali Mahjoory, Mohammadreza Kolahdouz, and Nima Taghavinia, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00970. keywords: {planar perovskite solar cell ETL Urea−SnO2 SCAPS interface}