daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Full Circle Recycling of Polysiloxanes via Room-Temperature Fluoride-Catalyzed Depolymerization to Repolymerizable Cyclics AITranslate

Bowling Green State University; Bowling Green State University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Siloxane-based polymeric materials are widely used all over the world because of their chemical, mechanical, and thermal stability and due to their low toxicity. Despite their usefulness, the high energy cost used to make them is lost when they are discarded, wasting resources and energy. Practical and simple methods of recycling these materials are therefore required. However, the simplification of these methods is underdeveloped. The present techniques used to recycle silicone-based materials, such as polydimethylsiloxanes, often involve high temperatures/pressures and complicated setups. To address this issue, we have established an efficient room-temperature technique for the depolymerization of silicone-based polymers, elastomers, and resins in the presence of low catalytic amounts of fluoride in specific high swell organic solvents. The products primarily contain cyclic siloxane units (D4, D5, and D6) as verified by GCMS and 29Si nuclear magnetic resonance. Nearly any silicone resin can be depolymerized rapidly using these methods. Silicone-rich systems result in the best conversions and the highest quantity of identifiable cyclics, while complex resins resulted in complicated products alongside discernible cyclics. We have also repolymerized the products from this process to reform silicones via acid, base, and fluoride catalysis. This process has the potential for large-scale industrial processing because of the use of mild conditions and solvent recycling ability.

KeyWords AITranslate

silicone depolymerization PDMS siloxane recycling green chemistry elastomers resins fluoride catalysis
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.0c01406

Chinese Library Classification Number:

Citation Information:

Siloxane-based polymeric materials are widely used all over the world because of their chemical, mechanical, and thermal stability and due to their low toxicity. Despite their usefulness, the high energy cost used to make them is lost when they are discarded, wasting resources and energy. Practical and simple methods of recycling these materials are therefore required. However, the simplification of these methods is underdeveloped. The present techniques used to recycle silicone-based materials, such as polydimethylsiloxanes, often involve high temperatures/pressures and complicated setups. To address this issue, we have established an efficient room-temperature technique for the depolymerization of silicone-based polymers, elastomers, and resins in the presence of low catalytic amounts of fluoride in specific high swell organic solvents. The products primarily contain cyclic siloxane units (D4, D5, and D6) as verified by GCMS and 29Si nuclear magnetic resonance. Nearly any silicone resin can be depolymerized rapidly using these methods. Silicone-rich systems result in the best conversions and the highest quantity of identifiable cyclics, while complex resins resulted in complicated products alongside discernible cyclics. We have also repolymerized the products from this process to reform silicones via acid, base, and fluoride catalysis. This process has the potential for large-scale industrial processing because of the use of mild conditions and solvent recycling ability.

quote

GB/T 7714-2015 [1] Buddhima Rupasinghe, Joseph C. Furgal. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01406.
MLA [1] Buddhima Rupasinghe, and Joseph C. Furgal. ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01406.
APA [1] Buddhima Rupasinghe, & Joseph C. Furgal. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01406
IEEE [1] Buddhima Rupasinghe and Joseph C. Furgal, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01406. keywords: {silicone depolymerization;PDMS;siloxane recycling;green chemistry;elastomers;resins;fluoride catalysis}