daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Study on the Agglomeration Mechanism of Nano-sized YSZ Synthesized with Hydrothermal Method AITranslate

School of Materials Science and Engineering, Hunan University;School of Materials Science and Engineering, Hunan University;School of Materials Science and Engineering, Hunan University;School of Materials Science and Engineering, Hunan University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Nano-sized powders were synthesized by hydrothermal method using ZrOCl4 ·8H20, Y(NO3)3 and ammonia as hydrotheraml precursor raw materials and water/mineralizer solutions as hydrothermal medium. The phase constitution and physical properties of YSZ powders were tested by the X-ray diffraction, scanning electron microscope and so on. The effects of hydrothermal process, the types and concentration of mineralizers,and organic surface activator on the agglomeration of nano-sized YSZ powders were in vestigated and some solutions were suggested accordingly.

KeyWords AITranslate

YSZ nano-sized powder hydrothermal method agglomeration

1Woo Seok Lee, Sun Woog Kim. Synthesis and microstructure of Y2 Oa-doped ZrO2-CeO2 composite nanoparticles by hydrothermal process[J]. Colloids and Surfaces A : Physicochemical and Engineering Aspects. 2008,313- 314..100-104.

2Piticescu R R, Monty C, Taloi D, et al. Hydrothermal synthesis of zirconia nanomaterials[J]. Journal of the European Ceramic Society,2001,21:2 057-2 060.

3Mater K. Surface'and catalytic properties of ZrO2 [J]. Chem Phys,1985,13(3-4) :347-364.

4邹兴.纳米粉制备过程中团聚现象的探讨[J].粉末冶金工业,2004,14(5):24-27. 被引量:12

5卓蓉晖.ZrO_2超细粉制备过程中粉体团聚的控制方法[J].江苏陶瓷,2002,35(3):32-33. 被引量:7

6胡英顺,尹秋响,侯宝红,王静康.结晶及沉淀过程中粒子聚结与团聚的研究进展[J].化学工业与工程,2005,22(5):371-375. 被引量:13

7陈少贞,林小莲.湿法制备ZrO_2超细粉的团聚机理、表征及控制[J].佛山陶瓷,1995(4):1-5. 被引量:3

8许小红.ZrO2(Y_2O_3)超细粉的制备及制备过程中团聚状态的控制[J].山西师大学报:自然科学版,1996,10(1):21-24. 被引量:1

9酒金婷,葛钥,张涑戎,李立平,屠凡,朱鹤孙.无团聚纳米氧化锆的制备及应用[J].无机材料学报,2001,16(5):867-871. 被引量:38

10许珂敬,许煜汾.表面活性剂在制备ZrO_2微粉中的作用[J].材料研究学报,1999,13(4):434-436. 被引量:40

1冯柳,魏春城,陈志伟.喷雾干燥法制备ZrO_2(3Y)微球[J].中国陶瓷,2010,46(7):31-32. 被引量:1

2赵多,孙本良.不同分散剂对水热法制备氧化锆颗粒分散性的影响[J].辽宁科技大学学报,2014,37(2):124-129.

3徐高峰,宋红章,杨德林.水热法制备稳定氧化锆纳米粉体[J].表面技术,2017,46(9):95-100. 被引量:3

4侯义飞,孙健,白妮,孙永芬,居殿春.基于响应曲面法的含锆废盐中ZrO_(2)的回收工艺[J].有色金属科学与工程,2021,12(6):26-34. 被引量:1

1刘旭恒,赵中伟,黄少波,张有新.喷雾干燥法合成球形LiFePO_4/C材料研究[J].电源技术,2012,36(7):937-941. 被引量:1

2周江峰,蔡东海,文东辉,尹林志.研抛加工机械加载力系统的设计与研究[J].机电工程,2018,35(8):853-856. 被引量:1

3傅小明,倪宗铭,方颖,杨在志,孙虎.M-ZrO2微球的制备及其光吸收特性[J].广州化工,2019,47(10):30-32.

4颜井意,郭心语,张雨,肖鑫,杜建周.氧化锆基结构陶瓷掺杂改性与增韧增强研究进展[J].当代化工研究,2023(2):174-178.

5甄杰,王宝祥,赵凯,陈伟,甄常亮,佟岩.基于响应曲面法的除尘灰与粉煤灰冷固结工艺优化[J].中国冶金,2023,33(7):130-136.

1宁宁.我国开发纳米氧化锆粉体制备新工艺[J].稀土信息,2002,8(2):14-14.

2Shuigen HUANG Kim VANMEENSEL Omer VAN DER BLEST Jozef VLEUGELS.Sintering, thermal stability and mechanical properties of ZrO2-WC composites obtained by pulsed electric current sintering[J].材料学前沿:英文版,2011,5(1):50-56.

3田猛,姜涛,刘卫强,杨芳,岳明,张久兴.放电等离子烧结纳米晶ZrO2陶瓷研究[J].功能材料,2004(z1):2717-2720. 被引量:1

4朱福兴,邓斌,秦庆东,王芳平.真空碳热还原制备碳氧钛的动力学研究[J].有色金属:冶炼部分,2014(3):46-50. 被引量:2

5王舟,陈肖虎,李东红,李武斌.纳米碳酸铝铵的制备[J].轻金属,2012(3):14-16. 被引量:2

6汤枫秋,黄校先,张玉峰,郭景坤.盐离子对纳米氧化锆浆料流变性能的影响[J].无机材料学报,1999,14(2):239-244. 被引量:8

7杨晓敏,闫翠芬,张晓芸,裴小苗,贾虎生,许并社.粉体表面包碳对3Y-TZP陶瓷烧结性能及微观结构的影响[J].材料导报,2005,19(11):122-124. 被引量:1

8周新木,赵光好,谈宏宇,徐招弟,李炳伟.纳米氧化锆的固相合成及机理研究[J].有色金属:冶炼部分,2006(1):50-53. 被引量:10

9陈祥歌,陈建铭,宋云华.三乙醇胺-水溶液介质水热合成纳米四方相氧化锆粉体[J].材料导报:纳米与新材料专辑,2011,25(1):130-132. 被引量:2

10刘曼朗.专利信息[J].粉末冶金工业,2007,17(5):56-56.

Basic Information:

DOI:

Chinese Library Classification Number:TF123.72[冶金工程—粉末冶金]

Citation Information:

Nano-sized powders were synthesized by hydrothermal method using ZrOCl4 ·8H20, Y(NO3)3 and ammonia as hydrotheraml precursor raw materials and water/mineralizer solutions as hydrothermal medium. The phase constitution and physical properties of YSZ powders were tested by the X-ray diffraction, scanning electron microscope and so on. The effects of hydrothermal process, the types and concentration of mineralizers,and organic surface activator on the agglomeration of nano-sized YSZ powders were in vestigated and some solutions were suggested accordingly.

quote

GB/T 7714-2015 [1] ZHU Bao-jun, TAO Ying, ZHANG Ting-ting, et al. Study on the Agglomeration Mechanism of Nano-sized YSZ Synthesized with Hydrothermal Method[J]. Rare Metals and Cemented Carbides, 2008(3): 1-5.
MLA [1] ZHU Bao-jun, et al., "Study on the Agglomeration Mechanism of Nano-sized YSZ Synthesized with Hydrothermal Method." Rare Metals and Cemented Carbides, no. 3, 2008, pp. 1-5.
APA [1] ZHU Bao-jun, TAO Ying, ZHANG Ting-ting, & DING Ying. (2008). Study on the Agglomeration Mechanism of Nano-sized YSZ Synthesized with Hydrothermal Method. Rare Metals and Cemented Carbides(3), 1-5.
IEEE [1] ZHU Bao-jun, TAO Ying, ZHANG Ting-ting, and DING Ying, "Study on the Agglomeration Mechanism of Nano-sized YSZ Synthesized with Hydrothermal Method," Rare Metals and Cemented Carbides, no. 3, pp. 1-5, 2008. keywords: {YSZ;nano-sized powder;hydrothermal method;agglomeration}