daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Research Progress and Challenges of Lithium Extraction from Salt Lake by Adsorption Method AITranslate

Zhongyuan Critical Metals Laboratory,Zhengzhou University;Zhongyuan Critical Metals Laboratory,Zhengzhou University;Zhongyuan Critical Metals Laboratory,Zhengzhou University;Zhongyuan Critical Metals Laboratory,Zhengzhou University;Zhongyuan Critical Metals Laboratory,Zhengzhou University;Zhongyuan Critical Metals Laboratory,Zhengzhou University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

With the rapid development of the global new energy industry,the demand for lithium has increased dramatically.Salt lake lithium resources with large reserves and low production costs have become the main source of lithium products.However,the development of lithium resources in salt lake is facing the double challenges of technology and environment,in which the separation of magnesium and lithium from brine with a high magnesium-lithium ratio is the key technical bottleneck.The adsorption method has attracted much attention in the field of lithium extraction from salt lake due to its advantages of strong adsorption capacity,high selectivity,simple preparation,low pollution and reusability of adsorbents.This paper reviews the research progress of the adsorption method for lithium extraction from salt lake,introduces the working principles and characteristics of inorganic adsorbents,organic adsorbents and composite adsorbents in detail,analyzes the problems and challenges faced by this method,and looks forward to its future development direction.

KeyWords AITranslate

salt lake brine lithium resource adsorption method magnesium-lithium separation
No data

Basic Information:

DOI:

Chinese Library Classification Number:TF826.3[冶金工程—有色金属冶金]

Citation Information:

With the rapid development of the global new energy industry,the demand for lithium has increased dramatically.Salt lake lithium resources with large reserves and low production costs have become the main source of lithium products.However,the development of lithium resources in salt lake is facing the double challenges of technology and environment,in which the separation of magnesium and lithium from brine with a high magnesium-lithium ratio is the key technical bottleneck.The adsorption method has attracted much attention in the field of lithium extraction from salt lake due to its advantages of strong adsorption capacity,high selectivity,simple preparation,low pollution and reusability of adsorbents.This paper reviews the research progress of the adsorption method for lithium extraction from salt lake,introduces the working principles and characteristics of inorganic adsorbents,organic adsorbents and composite adsorbents in detail,analyzes the problems and challenges faced by this method,and looks forward to its future development direction.

quote

GB/T 7714-2015 [1] DAI Yu, YANG Kai-hua, WU Shu-min, et al. Research Progress and Challenges of Lithium Extraction from Salt Lake by Adsorption Method[J]. Rare Metals and Cemented Carbides, 2025(6): 29-41.
MLA [1] DAI Yu, et al., "Research Progress and Challenges of Lithium Extraction from Salt Lake by Adsorption Method." Rare Metals and Cemented Carbides, no. 6, 2025, pp. 29-41.
APA [1] DAI Yu, YANG Kai-hua, WU Shu-min, REN Guo-xin, XU Wen-hua, & LIU Dong-fu. (2025). Research Progress and Challenges of Lithium Extraction from Salt Lake by Adsorption Method. Rare Metals and Cemented Carbides(6), 29-41.
IEEE [1] DAI Yu, YANG Kai-hua, WU Shu-min, REN Guo-xin, XU Wen-hua, and LIU Dong-fu, "Research Progress and Challenges of Lithium Extraction from Salt Lake by Adsorption Method," Rare Metals and Cemented Carbides, no. 6, pp. 29-41, 2025. keywords: {salt lake brine;lithium resource;adsorption method;magnesium-lithium separation}