daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Research Progress of the Second Phase Composition Modified Cemented Carbides AITranslate

School of Materials Science and Engineering,Hefei University of Technology;School of Materials Science and Engineering,Hefei University of Technology;School of Materials Science and Engineering,Hefei University of Technology;School of Materials Science and Engineering,Hefei University of Technology;School of Materials Science and Engineering,Hefei University of Technology;School of Materials Science and Engineering,Hefei University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The research progress of the second phase composition modified cemented carbides was systema-tically discussed,the modification mechanism,types of modifiers,and mechanical properties of WC-based cemented carbides modified by adding the second phase elements or compounds were introduced,and the improvement mechanism of mechanical properties of the cemented carbide by doping second phase was analyzed and summarized.The effect of modifying cemented carbides with different types and contents of additives is different.The effects of different additives and preparation methods on the mechanical properties of cemented carbides were classified and compared.The results show that the comprehensive mechanical properties of cemented carbides are mainly related to the degree of grain refinement and micro-interface structure.The added second phase can form a certain coordination structure with the WC matrix,effectively inhibit the growth of WC grains,and thus improve the performance of the alloy.Finally,the current development bottlenecks and unresolved issues of the second phase composition modified cemented carbides are summarized.

KeyWords AITranslate

cemented carbide second phase modification microstructure mechanical property

1吴涛.沥青黏结性影响因素研究[J].北方交通,2024(3):57-60.

2尹康,喻宁亚.一种环保型二氧化硅防锈颜料的制备及其应用[J].涂层与防护,2024,45(4):33-36.

3刘鑫,谯华,郭伟强,钱彦君,张书豪,朱龙辉.改性生物炭吸附固定环境中Cd(Ⅱ)/Pb(Ⅱ)的研究进展[J].绿色科技,2024,26(4):221-226.

4尤宏梅,陆佳,苏小红,刘伟.改性汉麻秸秆炭吸附亚甲基蓝性能研究[J].黑龙江科学,2024,15(12):97-100.

5刘文龙,董青岭.区块链问责:国际非政府组织的治理创新[J].复印报刊资料(国际政治),2023(11):106-115.

6王欣,刘兴伟,刘天宇,王玲,李树奎,熊宁,刘金旭.熔渗法制备W-Ce合金的探索研究[J].稀有金属材料与工程,2024,53(5):1363-1370.

7马力,魏振伟,周杰,李乐宇,邓志伟,范浩,彭文屹,刘昌奎.淬火水温对7050铝合金组织性能的影响[J].稀有金属材料与工程,2024,53(5):1262-1267.

8刘莉,羊求民,徐国钻,张龙辉,王红云,唐彦渊,钟远,林丽萍,邓同舟.混料方式对非均匀硬质合金微观结构及性能的影响[J].稀有金属与硬质合金,2024,52(3):84-90.

9罗春阳,徐流杰,申华海,李秀青,魏世忠.利用SRIM分析辐照对碳化物和氧化物陶瓷的影响[J].稀有金属材料与工程,2024,53(5):1245-1251.

10虞周楠,张磊磊,谈源龙,井日峥,曹宏晨,楼才溢,格日乐,王军虎,王爱琴,张涛.SnCl_(2)促进的Pt1/PS-PPh_(2)催化剂高选择性催化高碳烯烃氢甲酰化反应[J].Chinese Journal of Catalysis,2024,60(5):316-326.

Basic Information:

DOI:

Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]

Citation Information:

The research progress of the second phase composition modified cemented carbides was systema-tically discussed,the modification mechanism,types of modifiers,and mechanical properties of WC-based cemented carbides modified by adding the second phase elements or compounds were introduced,and the improvement mechanism of mechanical properties of the cemented carbide by doping second phase was analyzed and summarized.The effect of modifying cemented carbides with different types and contents of additives is different.The effects of different additives and preparation methods on the mechanical properties of cemented carbides were classified and compared.The results show that the comprehensive mechanical properties of cemented carbides are mainly related to the degree of grain refinement and micro-interface structure.The added second phase can form a certain coordination structure with the WC matrix,effectively inhibit the growth of WC grains,and thus improve the performance of the alloy.Finally,the current development bottlenecks and unresolved issues of the second phase composition modified cemented carbides are summarized.

quote

GB/T 7714-2015 [1] YANG Yu, ZHU Xiao-yong, ZAN Xiang, et al. Research Progress of the Second Phase Composition Modified Cemented Carbides[J]. Rare Metals and Cemented Carbides, 2024(3): 76-83.
MLA [1] YANG Yu, et al., "Research Progress of the Second Phase Composition Modified Cemented Carbides." Rare Metals and Cemented Carbides, no. 3, 2024, pp. 76-83.
APA [1] YANG Yu, ZHU Xiao-yong, ZAN Xiang, LUO Lai-ma, LIU Jia-qin, & WU Yu-cheng. (2024). Research Progress of the Second Phase Composition Modified Cemented Carbides. Rare Metals and Cemented Carbides(3), 76-83.
IEEE [1] YANG Yu, ZHU Xiao-yong, ZAN Xiang, LUO Lai-ma, LIU Jia-qin, and WU Yu-cheng, "Research Progress of the Second Phase Composition Modified Cemented Carbides," Rare Metals and Cemented Carbides, no. 3, pp. 76-83, 2024. keywords: {cemented carbide;second phase;modification;microstructure;mechanical property}