daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Experimental study on mix proportion of early-strength composite filling materials of full tailings paste AITranslate

Zhaoyuan Jiangjiayao Gold Mine Co.,Ltd.;Zhaoyuan Jiangjiayao Gold Mine Co.,Ltd.;Zhaoyuan Jiangjiayao Gold Mine Co.,Ltd.;Zhaoyuan Jiangjiayao Gold Mine Co.,Ltd.;Zhaoyuan Jiangjiayao Gold Mine Co.,Ltd.
AITranslate
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Mix proportion experiments were conducted on early-strength composite filling materials by employing full tailings as the main raw material to enhance the early strength of mine backfill and reduce filling costs.The physical and chemical properties of the full tailings were analyzed,and the compatibility of four types of early-strength agents with full tailings paste was evaluated,with the mix proportions of composite cementitious materials optimized by orthogonal experiments.The results show that the HY-3 early-strength agent performs best in improving early strength,increasing the 3-day strength by approximately 50%at a dosage of 1%.Without activators,the synergistic effect of clinker and mineral powder significantly enhances later-stage strength.In the system containing activators,the c4 formulation(45%clinker+40%mineral powder+10%quicklime+5%anhydrous sodium sulfate)achieves the 3-day,7-day,and 28-day compressive strength of 2.06 MPa,4.70 MPa,and 7.70 MPa respectively under the cement-sand ratio of 1∶6 and slurry concentration of 76%.This meets the mine’s false bottom strength requirement and enables low-cost replacement of traditional cement-based filling materials.The results can provide reliable technical support for low-cost,high-strength,and high-efficiency mine filling.

KeyWords AITranslate

full tailings paste filling early-strength agent composite cementitious material mix proportion optimization low-cost filling
No data

Basic Information:

DOI:

Chinese Library Classification Number:TD803[矿业工程—矿山开采]

Citation Information:

Mix proportion experiments were conducted on early-strength composite filling materials by employing full tailings as the main raw material to enhance the early strength of mine backfill and reduce filling costs.The physical and chemical properties of the full tailings were analyzed,and the compatibility of four types of early-strength agents with full tailings paste was evaluated,with the mix proportions of composite cementitious materials optimized by orthogonal experiments.The results show that the HY-3 early-strength agent performs best in improving early strength,increasing the 3-day strength by approximately 50%at a dosage of 1%.Without activators,the synergistic effect of clinker and mineral powder significantly enhances later-stage strength.In the system containing activators,the c4 formulation(45%clinker+40%mineral powder+10%quicklime+5%anhydrous sodium sulfate)achieves the 3-day,7-day,and 28-day compressive strength of 2.06 MPa,4.70 MPa,and 7.70 MPa respectively under the cement-sand ratio of 1∶6 and slurry concentration of 76%.This meets the mine’s false bottom strength requirement and enables low-cost replacement of traditional cement-based filling materials.The results can provide reliable technical support for low-cost,high-strength,and high-efficiency mine filling.

quote

GB/T 7714-2015 [1] Yang Tiejiang, Long Gang, Xu Tao, et al. Experimental study on mix proportion of early-strength composite filling materials of full tailings paste[J]. Gold, 2026(5): 46-52.
MLA [1] Yang Tiejiang, et al., "Experimental study on mix proportion of early-strength composite filling materials of full tailings paste." Gold, no. 5, 2026, pp. 46-52.
APA [1] Yang Tiejiang, Long Gang, Xu Tao, Liu Xiaosheng, & Xu Jing. (2026). Experimental study on mix proportion of early-strength composite filling materials of full tailings paste. Gold(5), 46-52.
IEEE [1] Yang Tiejiang, Long Gang, Xu Tao, Liu Xiaosheng, and Xu Jing, "Experimental study on mix proportion of early-strength composite filling materials of full tailings paste," Gold, no. 5, pp. 46-52, 2026. keywords: {full tailings;paste filling;early-strength agent;composite cementitious material;mix proportion optimization;low-cost filling}