Highly Sensitive Broad Light Response Organic Photodetectors from Pyrrolo[3,4-c]pyrrole-1,4-dione-Based Conjugated Polymer with Noncovalent Conformational Locks AITranslate

Lanzhou Jiaotong University; Lanzhou Jiaotong University; Lanzhou Jiaotong University; Lanzhou Jiaotong University; Lanzhou Jiaotong University; Lanzhou Jiaotong University; Lanzhou Jiaotong University; Lanzhou Jiaotong University; Harbin Institute of Technology; Lanzhou Jiaotong University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

An alternating narrow bandgap conjugated polymer named POT-DPP, comprising pyrrolo[3,4-c]pyrrole-1,4-dione (DPP) derivatives and 3,3′-dimethoxy-2,2′-bithiophene, was developed and successfully employ in organic photodiode detectors (OPDs). The polymer POT-DPP exhibited ampliative light absorption (from 300 to 1070 nm) in the solid state with an increased dielectric constant of 6.31 at 1 kHz, an upshifted highest occupied molecular orbital (HOMO) energy level (−4.98 eV), and increased planarity of conjugated molecules as compared to that of the polymer PDQT without methoxy side chains. The OPDs based on PDT-DPP:PC71BM blends, present high specific detectivity (D*) over 1013 Jones from 300 to 900 nm, a high linear dynamic range (LDR) of 153 dB, and response speed of about 86.6–90.4 μs. Moreover, the optimization of the OPDs was systematically implemented by replacing the ZnO cathode layer with a ZnO/PFN bilayer and modifying the photoactive layer thickness. The OPDs achieved the highest D* of 1.23 × 1014 Jones at 562 nm with a large high D*(over 1013) wavelength range from 300 to 900 nm with a 300 nm thick photoactive layer.

KeyWords AITranslate

organic photodiode detectors high sensitivity pyrrolo[3 4c]pyrrole1 4dione sidechain modification noncovalent conformational locks
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c00657

Chinese Library Classification Number:

Citation Information:

An alternating narrow bandgap conjugated polymer named POT-DPP, comprising pyrrolo[3,4-c]pyrrole-1,4-dione (DPP) derivatives and 3,3′-dimethoxy-2,2′-bithiophene, was developed and successfully employ in organic photodiode detectors (OPDs). The polymer POT-DPP exhibited ampliative light absorption (from 300 to 1070 nm) in the solid state with an increased dielectric constant of 6.31 at 1 kHz, an upshifted highest occupied molecular orbital (HOMO) energy level (−4.98 eV), and increased planarity of conjugated molecules as compared to that of the polymer PDQT without methoxy side chains. The OPDs based on PDT-DPP:PC71BM blends, present high specific detectivity (D*) over 1013 Jones from 300 to 900 nm, a high linear dynamic range (LDR) of 153 dB, and response speed of about 86.6–90.4 μs. Moreover, the optimization of the OPDs was systematically implemented by replacing the ZnO cathode layer with a ZnO/PFN bilayer and modifying the photoactive layer thickness. The OPDs achieved the highest D* of 1.23 × 1014 Jones at 562 nm with a large high D*(over 1013) wavelength range from 300 to 900 nm with a 300 nm thick photoactive layer.

quote

GB/T 7714-2015 [1] Yuan Zhou, Qian Wang, Pengzhi Guo, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00657.
MLA [1] Yuan Zhou, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00657.
APA [1] Yuan Zhou, Qian Wang, Pengzhi Guo, Xiaoqing You, Xianzheng Li, Shaotong Wang, Yi Liu, Chenglong Wang, Xianyu Deng, & Yangjun Xia. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00657
IEEE [1] Yuan Zhou, Qian Wang, Pengzhi Guo, Xiaoqing You, Xianzheng Li, Shaotong Wang, Yi Liu, Chenglong Wang, Xianyu Deng, and Yangjun Xia, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00657. keywords: {organic photodiode detectors high sensitivity pyrrolo[3;4c]pyrrole1;4dione sidechain modification noncovalent conformational locks}