The conditions of ash deposition and coking in waste heat utilization device of high-temperature flue gas from metallurgical furnaces are introduced.The mechanisms of physical and chemical coking of high-temperature flue gas and dust are analyzed.And the effective and practical specific measures are proposed to solve the coking problem of high-temperature flue gas and dust in waste heat utilization device.
KeyWords AITranslate
1李样人.闪速炉锅炉烟尘故障浅析[J].矿冶,2003,12(2):66-68. 被引量:7
2于强,张健强.燃用高钠煤对锅炉受热面的影响[J].锅炉制造,2012(4):4-6. 被引量:28
3阳绍伟,符慧林,黄文懋.挥发窑的余热利用[J].长沙水电师院学报:自然科学版,1995,10(4):387-393. 被引量:1
1曾锦波,卜文平.硅锰合金矿热炉烟气余热回收方法研究[J].中国资源综合利用,2022,40(7):81-83.
1夏盛,童敏,封羽涛.钢厂协同处置城市固体废弃物的实践与探索[J].广州化工,2017,45(18):138-140. 被引量:7
2朱中亮.一种升降式阀门装置的设计[J].设备管理与维修,2017(18):77-79.
3张卫东,施剑,曹春华,杨乙斌.AOD炉烟尘处理及余热回收技术开发应用[J].冶金动力,2018(1):36-41. 被引量:2
4王晨臣,彭孝天,王苏明,刘卫华,冯诗愚.燃油结焦影响因素及抑制方法综述[J].航空发动机,2018,44(2):64-69. 被引量:4
5孙晴亮,孙伟,龚长金.提升干熄焦装入装置集尘效果的措施[J].安徽冶金科技职业学院学报,2018,28(2):32-34.
6赵锋,薛占强,甘秀石,王健.高温检测装置在干熄炉的应用与实践[J].燃料与化工,2018,49(1):16-17.
7李乐,陈然,赵泽林.汽车排气管余热利用装置的创新设计分析[J].时代汽车,2018(8):84-85.
8提高产量、降低煤耗的旋风预热器试验成功[J].中国建材,1958,0(12):24-28.
9雷游生,黄天梁,邱秋生.氟化氢传统工艺装备的改进[J].厦门理工学院学报,2017,25(5):21-27. 被引量:1
10叶杰华.“学”成常态 “做”见实效[J].先锋,2016,0(12):65-65.
Basic Information:
DOI:
Chinese Library Classification Number:TF806[冶金工程—有色金属冶金]
Citation Information:
The conditions of ash deposition and coking in waste heat utilization device of high-temperature flue gas from metallurgical furnaces are introduced.The mechanisms of physical and chemical coking of high-temperature flue gas and dust are analyzed.And the effective and practical specific measures are proposed to solve the coking problem of high-temperature flue gas and dust in waste heat utilization device.
quote
| GB/T 7714-2015 | [1] TANG Zai-sheng, LIU Zhi-heng. Mechanism Analysis and Solution Discussion of High-temperature Flue Dust Coking in Metallurgical Furnaces[J]. Rare Metals and Cemented Carbides, 2018(4): 29-31. |
| MLA | [1] TANG Zai-sheng, and LIU Zhi-heng. "Mechanism Analysis and Solution Discussion of High-temperature Flue Dust Coking in Metallurgical Furnaces." Rare Metals and Cemented Carbides, no. 4, 2018, pp. 29-31. |
| APA | [1] TANG Zai-sheng, & LIU Zhi-heng. (2018). Mechanism Analysis and Solution Discussion of High-temperature Flue Dust Coking in Metallurgical Furnaces. Rare Metals and Cemented Carbides(4), 29-31. |
| IEEE | [1] TANG Zai-sheng and LIU Zhi-heng, "Mechanism Analysis and Solution Discussion of High-temperature Flue Dust Coking in Metallurgical Furnaces," Rare Metals and Cemented Carbides, no. 4, pp. 29-31, 2018. keywords: {high-temperature flue gas;high-temperature flue dust;eoking;mechanism;measure;metallurgical furnace;waste heat utilization device} |