Effect of Antimony on Performance of V-Mo/Ti Catalysts for Denitrification and Mercury Removal AITranslate
Abstract AITranslate
V-Mo-Sb/Ti catalyst was prepared by step impregnation method.XRD,XRF,N2-adsorption/desorption,NH3-TPD,H2-TPR,UV-Vis,and XPS were used to characterize the physicochemical properties of the catalyst.The denitrification performance and the oxidation activity of elemental mercury(Hg0)of the catalyst were evaluated by a fixed bed reactor.The results show that the loading of antimony leads to the increase of specific surface area,pore volume,surface acidity,reducibility and the content of chemi-sorbed oxygen of V-Mo/Ti catalyst,which improves the denitrification performance and the oxidation activity of Hg0.In addition,V-Mo-Sb/Ti catalyst also exhibits good resistance to SO2 and H2O.
KeyWords AITranslate
1赵彬,易红宏,唐晓龙,李倩,刘丁丁.燃煤烟气汞形态转化及脱除技术[J].现代化工,2015,35(1):58-62. 被引量:5
2胡鹏,段钰锋,陈亚南,周强,朱纯,丁卫科,李春峰,刘猛,王双群.Mo-Mn/TiO2催化剂的协同脱硝脱汞特性[J].中国环境科学,2018,38(2):523-531. 被引量:11
3耿新泽,段钰锋,胡鹏,柳帅,梁财.SCR气氛下Ce-W/TiO_2催化剂的脱硝协同脱汞特性[J].中国环境科学,2019,39(4):1419-1426. 被引量:8
4池桂龙,沈伯雄,朱少文,何川.改性SCR催化剂对单质汞氧化性能的研究[J].燃料化学学报,2016,44(6):763-768. 被引量:10
5李建荣,何炽,商雪松,陈进生,喻小伟,姚沅君.SCR脱硝催化剂对烟气中零价汞的氧化效率研究[J].燃料化学学报,2012,40(2):241-246. 被引量:22
6Chi Xu,Jian Liu,Zhen Zhao,Fei Yu,Kai Cheng,Yuechang Wei,Aijun Duan,Guiyuan Jiang.NH_3-SCR denitration catalyst performance over vanadium–titanium with the addition of Ce and Sb[J].环境科学学报:英文版,2015,0(5):74-80. 被引量:16
7晁晶迪,何洪,宋丽云,房玉娇,梁全明,张桂臻,邱文革,张然.Pr掺杂对V2O5-MoO3/TiO2催化剂NH3-SCR反应活性的影响[J].高等学校化学学报,2015,36(3):523-530. 被引量:30
8郭会宾,刘海刚,吴朝香,唐宏学.Sb_2O_3-CeO_2/TiO_2催化剂脱硝性能研究[J].应用化工,2019,48(5):1132-1135. 被引量:1
9刘欣,李俊华,李想,江晓明,王虎,李倩.工业VMoTi脱硝催化剂配方优化及氧化还原性研究[J].电力科技与环保,2016,32(1):6-9. 被引量:10
10程广文,张强,白博峰.一种改性选择性催化还原催化剂及其对零价汞的催化氧化性能[J].中国电机工程学报,2015,35(3):623-630. 被引量:16
1黄力,王虎,纵宇浩,常峥峰,刘洋,李金珂,韩沛.Cr对工业V-Mo/Ti脱硝催化剂的毒化作用研究[J].无机盐工业,2021,53(8):112-116. 被引量:2
2冼文琪,刘晓暄,刘保华,袁洁,谢正斌,区炜.聚碳酸亚丙酯二醇在聚氨酯中的应用研究进展[J].聚氨酯工业,2021,36(4):1-4. 被引量:5
3吴彦霞,王献忠,梁海龙,陈鑫,陈琛,戴长友,陈玉峰.钾盐沉积对VMoTi催化剂脱硝性能的影响[J].稀有金属材料与工程,2021,50(7):2343-2351. 被引量:2
4赵彤,赵斌彬,牛玉峰,梁瑜,刘雷,董晋湘,唐明兴,李学宽.不同结晶度的WO_(3)负载Pt低温催化萘加氢合成十氢萘[J].燃料化学学报,2021,49(8):1181-1189. 被引量:1
5刘宁,卢先明,王晓川,莫洪昌,张倩,李辉,徐明辉.新型非异氰酸酯固化体系研究进展[J].火炸药学报,2021,44(4):430-440. 被引量:2
6贾里,李泽鹏,郭晋荣,张永强,秦舒宁,王碧茹,樊保国,金燕.多元金属定向修饰的改性生物焦微观特性及单质汞脱除性能研究[J].环境科学学报,2021,41(8):3100-3111. 被引量:3
7钟雯,刘欢,王樱,付名利,吴军良,黄皓旻,叶代启,陈礼敏.载体结构对Co/MgO-Al_(2)O_(3)催化剂催化C_(2)H_(6)/CO_(2)反应性能的影响[J].环境科学学报,2021,41(8):3076-3088.
8李庆利.“三明治”型PTFE/Cu/炭黑/石墨气体扩散电极的制备及其电催化二氧化碳还原的性能研究[J].塑料科技,2021,49(7):34-37. 被引量:1
9薛琪,毕福强,王子俊,廉鹏,张家荣,吴敏杰,王伯周.1,3,4-噁二唑联呋咱含能化合物的设计及构效关系理论研究[J].火炸药学报,2021,44(4):461-467. 被引量:4
10张鹏,王继全,李源,姜丽莎,王壮壮,张高科.非贵金属助剂Ni_(2)P修饰类石墨碳氮化物光催化剂增强可见光光催化产氢性能[J].物理化学学报,2021,37(8):83-90. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:X511[环境科学与工程—环境工程]
Citation Information:
V-Mo-Sb/Ti catalyst was prepared by step impregnation method.XRD,XRF,N2-adsorption/desorption,NH3-TPD,H2-TPR,UV-Vis,and XPS were used to characterize the physicochemical properties of the catalyst.The denitrification performance and the oxidation activity of elemental mercury(Hg0)of the catalyst were evaluated by a fixed bed reactor.The results show that the loading of antimony leads to the increase of specific surface area,pore volume,surface acidity,reducibility and the content of chemi-sorbed oxygen of V-Mo/Ti catalyst,which improves the denitrification performance and the oxidation activity of Hg0.In addition,V-Mo-Sb/Ti catalyst also exhibits good resistance to SO2 and H2O.
quote
| GB/T 7714-2015 | [1] ZONG Yu-hao, LIU Yang, HUANG Li, et al. Effect of Antimony on Performance of V-Mo/Ti Catalysts for Denitrification and Mercury Removal[J]. Rare Metals and Cemented Carbides, 2021(4): 23-28. |
| MLA | [1] ZONG Yu-hao, et al., "Effect of Antimony on Performance of V-Mo/Ti Catalysts for Denitrification and Mercury Removal." Rare Metals and Cemented Carbides, no. 4, 2021, pp. 23-28. |
| APA | [1] ZONG Yu-hao, LIU Yang, HUANG Li, WANG Hu, CHANG Zheng-feng, GAO Yi-bo, & LI Jin-ke. (2021). Effect of Antimony on Performance of V-Mo/Ti Catalysts for Denitrification and Mercury Removal. Rare Metals and Cemented Carbides(4), 23-28. |
| IEEE | [1] ZONG Yu-hao, LIU Yang, HUANG Li, WANG Hu, CHANG Zheng-feng, GAO Yi-bo, and LI Jin-ke, "Effect of Antimony on Performance of V-Mo/Ti Catalysts for Denitrification and Mercury Removal," Rare Metals and Cemented Carbides, no. 4, pp. 23-28, 2021. keywords: {V-Mo/Ti catalyst;antimony;denitrification;mercury removal} |