Preparation of Al-Sc Intermediate Alloy by Alumino-thermic Reduction of Sc_2O_3 AITranslate

Hunan Rare Earth Metal Material Research Institute;Hunan Rare Earth Metal Material Research Institute;Hunan Rare Earth Metal Material Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Al-Sc intermediate alloy is prepared by alumino-thermic reduction. The test results showed that the addition of appropriate amount of ScF3 into nNaF · AlF3-KCl-NaCl molten salt can improve Sc2O3 solubility;the use of liquid A1 as reductant for the preparation of Al-Sc intermediate alloy can increase Sc content (assaying 2% mass)and Sc recovery as well as improve the quality of the intermediate alloy and reduce the operating cost,as can facilitate the further application of Al-Sc intermediate alloy.

KeyWords AITranslate

alumino-thermic red uction Sc2O3 preparation Al-Sc intermediate alloy

1姜锋,尹志民,李汉广.铝钪中间合金的制备方法[J].稀土,2001,22(1):41-44. 被引量:26

2杨庆山,李中华,柳术平,贺丰收,刘甲祥.Al-Sc中间合金制备技术及研发方向[J].湖南有色金属,2006,22(1):42-44. 被引量:8

3尹志民,李汉广,姜锋.钪和含钪合金[M].长沙:中南大学出版社,2001.128.

4孙本良,翟玉春,田彦文.氟盐体系中电解制取铝钪合金的研究[J].稀有金属,1998,22(3):191-194. 被引量:23

5黄美松.铝-钪(2%)合金的制备[J].江西有色金属,2005,19(2):28-31. 被引量:9

6路贵民,刘学山.冰晶石熔体中Al热还原法制备Al-Sc合金[J].中国有色金属学报,1999,9(1):171-174. 被引量:22

7路贵民,刘学山.氧化钪在nNaF·AlF_3ScF_3熔盐体系中的溶解[J].中国有色金属学报,1999,9(3):624-626. 被引量:24

1豆志河,张廷安,姚建明,蒋孝丽,牛丽萍,赫冀成.Al_2O_3-CaO熔渣性能的研究[J].过程工程学报,2009,9(S1):246-249. 被引量:9

2苏正夫,包新军,王志坚,刘吉波,吴希桃,邓志军.从包钢选矿厂尾矿中回收粗氧化钪的工艺研究[J].中国有色冶金,2015,44(1):60-62. 被引量:4

3林德源,李一,陈云翔,蔡建宾,郑勇.稀土在铝合金防腐中的应用[J].稀土,2016,37(6):121-127. 被引量:11

4甘培原,何航军,谢营邦,詹海鸿,刘晨.NaF-NaCl-KCl-ScF_3熔盐体系中铝热还原Sc_2O_3制备Al-Sc中间合金[J].稀有金属与硬质合金,2016,44(6):49-53. 被引量:2

5李亮星,王涛胜,黄茜琳,黄金堤.熔盐电解法制备铝钪中间合金研究进展[J].材料导报,2018,32(21):3768-3773. 被引量:8

6柳旭,王炜,元琳琳,王峰.放电等离子烧结快速制备高钪含量铝钪合金[J].粉末冶金技术,2020,38(2):126-131. 被引量:2

1史冠勇,张廷安,牛丽萍,豆志河.低氟CaF_2-CaO-Al_2O_3-MgO-SiO_2系精炼渣的性能[J].过程工程学报,2011,11(4):695-700. 被引量:15

2宋玉环.铝热还原生产钒铁合金的工艺优化[J].中国科技博览,2012(7):104-104.

3李丽,马成骥,张京叶.铝合金表面化学转化技术的研究进展[J].材料保护,2019,52(1):113-117. 被引量:5

4任耘,孙璐艳,赵福才,冯璐,巨建涛.CaF_2及碱度变化对中间包覆盖剂黏度的影响[J].钢铁研究学报,2015,27(1):35-39. 被引量:5

5杨波,陈国银,丁文捷.高钒铁精炼过程中自动喷吹装置的研究与应用[J].铁合金,2015,46(3):36-40.

6刘立,赵俊学,李献民,丁五洲,陈峰,李小孟.CaF_2-CaO-Al_2O_3-SiO_2-MgO五元渣的表面张力及其在镍基合金电渣重熔的应用[J].特殊钢,2015,36(6):20-22. 被引量:4

7郭志超,刘轩,薛济来,张鹏举.超声对熔盐电解法制备Al--7Si--Sc合金组织的影响[J].工程科学学报,2019,0(9):1135-1141. 被引量:5

8向燕,郑鑫,张蔚,曾文华,刘红霞,张小联.KF-AlF_3-Sc_2O_3熔盐体系下沉阴极法制备Al-Sc合金的实验研究[J].稀有金属与硬质合金,2018,46(2):37-41. 被引量:4

9邹小琴,刘壮壮,李慕华,张华文.铝稀土涂层制备及其防腐性能试验研究[J].黄金,2018,39(5):4-7.

10张赛楠,潘利文,罗涛,黄丹琳,董强,胡治流.稀土La和Ce及超声处理对ZL201铝合金显微组织及抗拉强度的影响[J].材料导报,2018,32(14):2452-2457. 被引量:5

1何碧宁,杨庆山,柳术平,陈卫平,刘甲祥,张卫平.ScF_3冰晶石熔盐体系中铝热还原Sc_2O_3制备Al—Sc中间合金[J].湖南冶金,2006,34(3):9-12. 被引量:3

2唐冲冲,常化强,包晓刚,刘贵清,刘奎仁.铝锶热还原Sc_2O_3制备铝钪中间合金[J].中国稀土学报,2012,30(6):680-685. 被引量:6

3甘培原,何航军,谢营邦,詹海鸿,刘晨.NaF-NaCl-KCl-ScF_3熔盐体系中铝热还原Sc_2O_3制备Al-Sc中间合金[J].稀有金属与硬质合金,2016,44(6):49-53. 被引量:2

4杨庆山,李中华,柳术平,贺丰收,刘甲祥.Al-Sc中间合金制备技术及研发方向[J].湖南有色金属,2006,22(1):42-44. 被引量:8

5谷兰成.Al-Ti-B中间合金夹渣的形成机理及清除[J].轻合金加工技术,2001,29(9):10-12. 被引量:4

6田忠良,杨树,赖延清,胡勋,张腾.熔盐电解法制备铝-钪中间合金的研究进展[J].矿产保护与利用,2013,33(5):55-58. 被引量:4

7路贵民,刘学山.冰晶石熔体中Al热还原法制备Al-Sc合金[J].中国有色金属学报,1999,9(1):171-174. 被引量:22

8李广宇,杨少华,李继东,胡宪伟,王兆文,张明杰,邱竹贤.熔盐电解法制备铝钪合金的研究[J].轻金属,2007(5):54-57. 被引量:8

9马柏祥.优化nNaF·AlF3—Al2O3—MgF2系熔体实晶温度的数学模型[J].铝镁通讯,1999(2):32-34.

10姜锋,尹志民,李汉广,潘青林,彭志辉,阿列克桑德夫斯基 С В,拉特涅尔 A X.氧化钪-氯化-铝镁热还原法制备钪中间合金新工艺研究[J].稀土,2001,22(3):34-36. 被引量:5

Basic Information:

DOI:

Chinese Library Classification Number:TG803.131[金属学及工艺—公差测量技术];TF845.1[冶金工程—有色金属冶金]

Citation Information:

Al-Sc intermediate alloy is prepared by alumino-thermic reduction. The test results showed that the addition of appropriate amount of ScF3 into nNaF · AlF3-KCl-NaCl molten salt can improve Sc2O3 solubility;the use of liquid A1 as reductant for the preparation of Al-Sc intermediate alloy can increase Sc content (assaying 2% mass)and Sc recovery as well as improve the quality of the intermediate alloy and reduce the operating cost,as can facilitate the further application of Al-Sc intermediate alloy.

quote

GB/T 7714-2015 [1] YANG Qing-shan, CHEN Jian-jun, CHEN Wei-ping. Preparation of Al-Sc Intermediate Alloy by Alumino-thermic Reduction of Sc_2O_3[J]. Rare Metals and Cemented Carbides, 2007(2): 5-7.
MLA [1] YANG Qing-shan, et al., "Preparation of Al-Sc Intermediate Alloy by Alumino-thermic Reduction of Sc_2O_3." Rare Metals and Cemented Carbides, no. 2, 2007, pp. 5-7.
APA [1] YANG Qing-shan, CHEN Jian-jun, & CHEN Wei-ping. (2007). Preparation of Al-Sc Intermediate Alloy by Alumino-thermic Reduction of Sc_2O_3. Rare Metals and Cemented Carbides(2), 5-7.
IEEE [1] YANG Qing-shan, CHEN Jian-jun, and CHEN Wei-ping, "Preparation of Al-Sc Intermediate Alloy by Alumino-thermic Reduction of Sc_2O_3," Rare Metals and Cemented Carbides, no. 2, pp. 5-7, 2007. keywords: {alumino-thermic red uction;Sc2O3;preparation;Al-Sc intermediate alloy}