Bionic Shape Memory Polyurethane/Prussian Blue Nanoparticle-Based Actuators with Two-Way and Programmable Light-Driven Motions AITranslate
Abstract AITranslate
A bionic smart actuator that can imitate types of biological motions plays a vital role in intelligent systems, which therefore becomes one of the hottest development directions in recent years and has attracted more and more attention from researchers. In this study, a kind of near-infrared (NIR) light-responsive shape memory polyurethane SMPU-PB is developed by doping the citric acid-modified Prussian blue nanoparticles. Based on it, a bionic “athlete” has performed repeatable photomechanical jumping behavior to cross obstacles under 808 nm NIR light irradiation. Furthermore, through the integration of SMPU-PB with pre-strained UV-responsive polyurethane film, a hybrid wavelength-selective responsive structure capable of reversible, programmable, and controllable motions is produced. By using the two-way light-driven shape memory composite, the bionic actuator is able to complete a series of tasks including accurate bending and mechanical gripping.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.2c01911
Chinese Library Classification Number:
Citation Information:
A bionic smart actuator that can imitate types of biological motions plays a vital role in intelligent systems, which therefore becomes one of the hottest development directions in recent years and has attracted more and more attention from researchers. In this study, a kind of near-infrared (NIR) light-responsive shape memory polyurethane SMPU-PB is developed by doping the citric acid-modified Prussian blue nanoparticles. Based on it, a bionic “athlete” has performed repeatable photomechanical jumping behavior to cross obstacles under 808 nm NIR light irradiation. Furthermore, through the integration of SMPU-PB with pre-strained UV-responsive polyurethane film, a hybrid wavelength-selective responsive structure capable of reversible, programmable, and controllable motions is produced. By using the two-way light-driven shape memory composite, the bionic actuator is able to complete a series of tasks including accurate bending and mechanical gripping.
quote
| GB/T 7714-2015 | [1] Xiaofei Wang, Yang He, Jinsong Leng. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c01911. |
| MLA | [1] Xiaofei Wang, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c01911. |
| APA | [1] Xiaofei Wang, Yang He, & Jinsong Leng. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c01911 |
| IEEE | [1] Xiaofei Wang, Yang He, and Jinsong Leng, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c01911. keywords: {Prussian blue nanoparticles;reversible shape memory composite;jumping athlete;bionic actuators;programmable motions} |