Study on the Tin Behavior and Tin Removal in Tungsten Hydrometallurgy AITranslate
Abstract AITranslate
The behavior of tin in tungsten hydrometallurgy is analyzed, and a co-precipitation method is presented for removal of impurity element tin from Na2WO4 solution. The effect of H2O2 and reagent A addition is studied.
KeyWords AITranslate
1谭光华,袁廉灼.高杂Na_2WO_4溶液制取优质APT[J].稀有金属与硬质合金,1990(3):19-21. 被引量:4
2李洪桂,李运姣,孙培梅,刘茂盛.钨矿物原料NaOH分解过程中抑制杂质的研究[J].中国工程科学,2000,2(3):59-61. 被引量:13
3尹树普,李志国,贺志超.湿冶离子交换法生产仲钨酸铵工艺中杂质锡的行为[J].中国钨业,2002,17(2):27-29. 被引量:12
1康金华.环烷酸-盐酸体系中料液的除杂研究[J].南方冶金学院学报,2004,25(1):25-28. 被引量:2
2冷明锋.吸附共沉淀法分离钼酸铵中的钨[J].中国钼业,2011,35(2):36-38. 被引量:3
3尹树普,李志国,贺志超.湿冶离子交换法生产仲钨酸铵工艺中杂质锡的行为[J].中国钨业,2002,17(2):27-29. 被引量:12
4刘斌莲,王宝军,李良东.铅电解粗铅精炼过程中除锡的生产实践[J].有色矿冶,2013,29(2):35-36. 被引量:2
5涂相林.分碲液除锡的研究[J].铜业工程,2011(3):29-30. 被引量:1
6王世文.粗铅精炼过程中除锡的研究[J].有色矿冶,1998,14(6):31-34.
7刘猛,杨飞,黄文孝,吴金玲.从ITO靶材中提取高纯度铟实验研究[J].山东化工,2017,46(6):18-19. 被引量:3
8汪祚敬.浅谈用系统方法降低钨冶炼过程中的不良品率[J].稀有金属与硬质合金,1993,21(S1):397-401.
9冶金过程强化学科组.“选择性沉淀法从钨酸盐溶液中除钼、砷、锡、锑”专利技术的新进展[J].中国钨业,2000,15(4):29-30. 被引量:7
10洪代琳.仲胺类萃取在我厂的应用[J].中国钨业,1996,11(10):27-29.
Basic Information:
DOI:
Chinese Library Classification Number:TF803.25[冶金工程—有色金属冶金]
Citation Information:
The behavior of tin in tungsten hydrometallurgy is analyzed, and a co-precipitation method is presented for removal of impurity element tin from Na2WO4 solution. The effect of H2O2 and reagent A addition is studied.
quote
| GB/T 7714-2015 | [1] JIANG Wen-wei, ZHAO Zhong-wei, LIANG Wei-dong, et al. Study on the Tin Behavior and Tin Removal in Tungsten Hydrometallurgy[J]. Rare Metals and Cemented Carbides, 2008(3): 38-42. |
| MLA | [1] JIANG Wen-wei, et al., "Study on the Tin Behavior and Tin Removal in Tungsten Hydrometallurgy." Rare Metals and Cemented Carbides, no. 3, 2008, pp. 38-42. |
| APA | [1] JIANG Wen-wei, ZHAO Zhong-wei, LIANG Wei-dong, & ZHAO Ling-ping. (2008). Study on the Tin Behavior and Tin Removal in Tungsten Hydrometallurgy. Rare Metals and Cemented Carbides(3), 38-42. |
| IEEE | [1] JIANG Wen-wei, ZHAO Zhong-wei, LIANG Wei-dong, and ZHAO Ling-ping, "Study on the Tin Behavior and Tin Removal in Tungsten Hydrometallurgy," Rare Metals and Cemented Carbides, no. 3, pp. 38-42, 2008. keywords: {tungsten metallurgy Na2 WO4 solution tin removal absorption co-precipitation} |