Bi2O2Se/Xene for Steep-Slope Transistors Bi2O2Se/Xene for Steep-Slope Transistors AITranslate
Abstract AITranslate
Thanks to the unique properties of two-dimensional (2D) materials and their van der Waals (vdW) heterostructures, 2D materials technologies have continued to make big strides. Among various 2D materials semiconductors, the recently discovered bismuth oxyselenide (Bi2O2Se) is highly attractive because of its high electron mobility, air stability, as well as its ability to form native high-k oxide. Combined with semi-metallic graphene, the Bi2O2Se/graphene heterostructure has been shown to excel in optoelectronic and electronic applications. Herein, we unveil and demonstrate a new application potential of Bi2O2Se/Xene heterostructures for making steep-slope transistors, as urgently required in the face of an increasingly challenging power issue. Atomic-scale materials simulations reveal that nearly Ohmic contact is formed between Bi2O2Se and Xene (graphene and silicene). In forming the heterointerface, Xene is p-type doped with the Fermi level in the lower Dirac cone where density of states of electrons is a decreasing function of energy. This property and the high electrostatic controllability of the barrier height at the vdW interface naturally satisfy the material requirements of the steep-slope “cold-source” transistor. Device modelings confirm that the n-type Bi2O2Se transistor with graphene or silicene as the source is indeed a steep-slope transistor, with a room-temperature sub-threshold swing below 50 mV/decade. Compared to normal Bi2O2Se transistor and steep-slope tunneling transistor, the “cold-source” Bi2O2Se transistor also exhibits a higher drive current. This work provides an atomistic understanding of Bi2O2Se/Xene-based steep-slope transistors and opens a new direction in precision vdW contact engineering toward achieving nanoscale electronic devices for applications in a low-power integrated circuit.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.3c00530
Chinese Library Classification Number:
Citation Information:
Thanks to the unique properties of two-dimensional (2D) materials and their van der Waals (vdW) heterostructures, 2D materials technologies have continued to make big strides. Among various 2D materials semiconductors, the recently discovered bismuth oxyselenide (Bi2O2Se) is highly attractive because of its high electron mobility, air stability, as well as its ability to form native high-k oxide. Combined with semi-metallic graphene, the Bi2O2Se/graphene heterostructure has been shown to excel in optoelectronic and electronic applications. Herein, we unveil and demonstrate a new application potential of Bi2O2Se/Xene heterostructures for making steep-slope transistors, as urgently required in the face of an increasingly challenging power issue. Atomic-scale materials simulations reveal that nearly Ohmic contact is formed between Bi2O2Se and Xene (graphene and silicene). In forming the heterointerface, Xene is p-type doped with the Fermi level in the lower Dirac cone where density of states of electrons is a decreasing function of energy. This property and the high electrostatic controllability of the barrier height at the vdW interface naturally satisfy the material requirements of the steep-slope “cold-source” transistor. Device modelings confirm that the n-type Bi2O2Se transistor with graphene or silicene as the source is indeed a steep-slope transistor, with a room-temperature sub-threshold swing below 50 mV/decade. Compared to normal Bi2O2Se transistor and steep-slope tunneling transistor, the “cold-source” Bi2O2Se transistor also exhibits a higher drive current. This work provides an atomistic understanding of Bi2O2Se/Xene-based steep-slope transistors and opens a new direction in precision vdW contact engineering toward achieving nanoscale electronic devices for applications in a low-power integrated circuit.
quote
| GB/T 7714-2015 | [1] Juan Lyu, Shun Song, Jian Gong. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00530. |
| MLA | [1] Juan Lyu, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00530. |
| APA | [1] Juan Lyu, Shun Song, & Jian Gong. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00530 |
| IEEE | [1] Juan Lyu, Shun Song, and Jian Gong, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00530. keywords: {Bi2O2Se/Xene heterostructures coldsource Dirac semimetal the subthreshold slope onstate current} |