Hyper-Cross-Linked Nanoparticle Reinforced Composite Polymer Electrolytes with Enhanced Ionic Conductivity and Thermal Stability for Lithium-Ion Batteries AITranslate

Sichuan University; Sichuan University; Sichuan University; Sichuan University; Sichuan University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Solid polymer electrolytes (SPEs) have been considered as promising substitutes for liquid electrolytes in lithium-ion batteries due to their flexibility and nonflammability. However, there are still significant challenges to be overcome, such as the low ion conductivity and undesirable lithium ion transference number (tLi+). In this study, we prepare poly(ethylene oxide)-based composite solid polymer electrolytes (CSPE-HCPs) using hyper-cross-linked SiO2@PMMA-co-PS nanoparticles as the reinforcement. In contrast to the conventional SPEs, CSPE-HCPs can maintain dimensional thermal stability up to 260 °C. Meanwhile, the ionic conductivity of CSPE-HCPs can be up to 1.13 × 10–4 S cm–1 at 30 °C and the tLi+ can reach 0.51 at room temperature due to the porous hyper-cross-linked polymeric shell. Furthermore, LiFePO4/CSPEs/Li cells possess excellent rate performance and relatively stable cycle performance in addition to their outstanding electrochemical window (up to 5.3 V). It is demonstrated that these solid electrolytes reinforced by hyper-cross-linked composite nanoparticles can be a promising component to improve the performance of all solid-state lithium-ion batteries.

KeyWords AITranslate

hypercrosslinked network Friedelcrafts alkylation reaction organic−inorganic composite nanoparticles solid polymer electrolytes Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01997

Chinese Library Classification Number:

Citation Information:

Solid polymer electrolytes (SPEs) have been considered as promising substitutes for liquid electrolytes in lithium-ion batteries due to their flexibility and nonflammability. However, there are still significant challenges to be overcome, such as the low ion conductivity and undesirable lithium ion transference number (tLi+). In this study, we prepare poly(ethylene oxide)-based composite solid polymer electrolytes (CSPE-HCPs) using hyper-cross-linked SiO2@PMMA-co-PS nanoparticles as the reinforcement. In contrast to the conventional SPEs, CSPE-HCPs can maintain dimensional thermal stability up to 260 °C. Meanwhile, the ionic conductivity of CSPE-HCPs can be up to 1.13 × 10–4 S cm–1 at 30 °C and the tLi+ can reach 0.51 at room temperature due to the porous hyper-cross-linked polymeric shell. Furthermore, LiFePO4/CSPEs/Li cells possess excellent rate performance and relatively stable cycle performance in addition to their outstanding electrochemical window (up to 5.3 V). It is demonstrated that these solid electrolytes reinforced by hyper-cross-linked composite nanoparticles can be a promising component to improve the performance of all solid-state lithium-ion batteries.

quote

GB/T 7714-2015 [1] Caimei Yu, Xue Gong, Mengyang Wang, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c01997.
MLA [1] Caimei Yu, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c01997.
APA [1] Caimei Yu, Xue Gong, Mengyang Wang, Longyu Li, & Shijie Ren. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c01997
IEEE [1] Caimei Yu, Xue Gong, Mengyang Wang, Longyu Li, and Shijie Ren, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c01997. keywords: {hypercrosslinked network;Friedelcrafts alkylation reaction;organic−inorganic composite nanoparticles;solid polymer electrolytes;Show More}