Abstract AITranslate

Statistical copolymers of methacrylic acid (MAA) and methyl methacrylate (MMA), butyl methacrylate (BMA), or lauryl methacrylate (LMA) were synthesized via cobalt(II)-mediated catalytic chain transfer polymerization (CCTP) and used as macromonomeric stabilizers in the emulsion polymerization of MMA. By varying the composition, length, and concentration of the macromonomers, we were able to tune the particle size, molar mass, and rheological behavior of the latexes. Most latexes stabilized with macromonomers containing BMA and LMA showed rheological properties such as small yield stress and shear thinning behavior similar to those of binders for coating applications.

KeyWords AITranslate

emulsion polymerization reactive surfactant methacrylic acid copolymerization macromonomer catalytic chain transfer
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00715

Chinese Library Classification Number:

Citation Information:

Statistical copolymers of methacrylic acid (MAA) and methyl methacrylate (MMA), butyl methacrylate (BMA), or lauryl methacrylate (LMA) were synthesized via cobalt(II)-mediated catalytic chain transfer polymerization (CCTP) and used as macromonomeric stabilizers in the emulsion polymerization of MMA. By varying the composition, length, and concentration of the macromonomers, we were able to tune the particle size, molar mass, and rheological behavior of the latexes. Most latexes stabilized with macromonomers containing BMA and LMA showed rheological properties such as small yield stress and shear thinning behavior similar to those of binders for coating applications.

quote

GB/T 7714-2015 [1] Ingeborg SchreurPiet, Johan P.A. Heuts. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00715.
MLA [1] Ingeborg SchreurPiet, and Johan P.A. Heuts. ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00715.
APA [1] Ingeborg SchreurPiet, & Johan P.A. Heuts. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00715
IEEE [1] Ingeborg SchreurPiet and Johan P.A. Heuts, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00715. keywords: {emulsion polymerization;reactive surfactant;methacrylic acid;copolymerization;macromonomer;catalytic chain transfer}