Study on Microstructure and Properties of Laser Cladding(FeCrCo/Ni)_5-SiTiNbMoW High-entropy Alloy Coatings AITranslate

Department of Mechanical and Electronic Engineering,Guizhou Communication Vocational College;Department of Mechanical and Electronic Engineering,Guizhou Communication Vocational College;Department of Mechanical and Electronic Engineering,Guizhou Communication Vocational College;Department of Mechanical and Electronic Engineering,Guizhou Communication Vocational College;Department of Mechanical and Electronic Engineering,Guizhou Communication Vocational College;Department of Mechanical and Electronic Engineering,Guizhou Communication Vocational College
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The (FeCrCo/Ni)5-SiTiNbMoW high-entropy alloy coatings were successfully prepared on the surface of the tool steel by laser cladding technology. The microstructure,composition, phase and hardness of the coatings were analyzed and tested by SEM/EDS, XRD and microhardness tester. The results show that the (FeCrCo)5-SiTiNbMoW coating contains BCC main phase,and a small amount of MC phase and Laves phase. The (FeCrNi)5-SiTiNbMoW coating contains FCC main phase and a small amount of MC phase and Laves phase. The two coatings are dominated by dendrites,while the (FeCrNi)5-SiTiNbMoW coating also has eutectic microstructure. The microhardness of the (FeCrCo)5-SiTiNbMoW high-entropy alloy coating is slightly higher than that of the (FeCrNi)5-SiTiNbMoW high-entropy alloy coating.

KeyWords AITranslate

high entropy alloy coating laser cladding microstructure phase hardness

1梁秀兵,魏敏,程江波,张伟,徐滨士.高熵合金新材料的研究进展[J].材料工程,2009,37(12):75-79. 被引量:72

2尚建路,程从前,王锐,祝志超,赵杰.AlCrFeNi多主元高熵合金的高温性能[J].机械工程材料,2014,38(2):72-75. 被引量:9

3李安敏,张喜燕,刘乐林,郑良杰.退火对AlCrFeCoNiCu高熵合金组织与性能的影响[J].机械工程材料,2012,36(7):14-16. 被引量:7

4张冲,吴炳乾,王乾廷,陈鼎宁,戴品强.激光熔覆FeCrNiCoMnB_x高熵合金涂层的组织结构与性能[J].稀有金属材料与工程,2017,46(9):2639-2644. 被引量:26

5王志坚,董世运,徐滨士,夏伟.激光熔覆工艺参数对金属成形效率和形状的影响[J].红外与激光工程,2010,39(2):315-319. 被引量:26

6邹朋津,董刚,王梁,姚建华.激光熔覆制备CrNiAlCoMoB0.5高熵合金涂层的组织与耐腐蚀性能研究[J].中国激光,2015,0(B09):117-123. 被引量:1

7张勇,周云军,陈国良.快速发展中的高熵溶体合金[J].物理,2008,37(8):600-605. 被引量:31

8邱星武,刘春阁,张云鹏.激光熔覆Al_2CoCrCuFeNi_xTi高熵合金涂层的组织及性能[J].激光与光电子学进展,2017,54(5):261-267. 被引量:7

9邱星武,张云鹏,刘春阁.激光熔覆法制备Al_2CrFeCo_xCuNiTi高熵合金涂层的组织与性能[J].粉末冶金材料科学与工程,2013,18(5):735-740. 被引量:38

10何力,张云鹏,邱星武.Al_2CrFeNiCo_xCuTi高熵合金的组织结构及腐蚀性能研究[J].稀有金属与硬质合金,2013,41(4):38-41. 被引量:9

1韩雪莹,刘新利,吴壮志,段柏华,王德志.含难熔金属涂层的研究进展[J].材料导报,2020,34(13):13146-13154. 被引量:3

2安亚君,芦晶晶,曹皓崴.稀土含量对活性激光熔覆Fe-Cr-W-Ni-C涂层的组织和磨损性能的影响[J].材料保护,2020,53(3):101-106. 被引量:5

3贾智轩,褚延朋,冯运莉,李杰.高熵合金制备及热处理工艺研究进展[J].金属热处理,2020,45(10):17-23. 被引量:11

4傅康,王俊,王帅.磁控溅射功率对半导体硅基表面FeCrNi涂层组织及性能的影响[J].真空科学与技术学报,2020,40(10):897-901.

5赵堃,冯小明,艾桃桃.高熵合金典型微观结构和性能研究进展[J].陕西理工大学学报:自然科学版,2021,37(2):1-8. 被引量:1

6夏铭,孙博,王鑫,梁秀兵,沈宝龙.高熵合金增材制造研究现状与展望[J].材料导报,2021,35(13):13119-13127. 被引量:3

1刘卫东,米国发,李雷.合金成分对激光熔覆高熵合金涂层影响的研究进展[J].特种铸造及有色合金,2022,42(7):847-855.

2姚海睿,张盼盼.高温合金热处理工艺研究进展[J].信息记录材料,2021,22(3):5-6.

3武雅桃,黄德军,杨慧君,张敏,乔珺威.不完全再结晶Fe_(40)Mn_(10)Cr_(25)Ni_(25)高熵合金的室温及低温力学性能[J].金属热处理,2021,46(6):160-167. 被引量:1

4田浩亮,张晓敏,金国,朴钟宇,王长亮,郭孟秋,杜修忻,王天颖,张昂,肖晨兵.电火花沉积高熵合金涂层的研究现状与展望[J].材料导报,2021,35(S01):342-346. 被引量:3

5姚芳萍,房立金,李金华,冯伟龙.Y_(2)O_(3)对激光熔覆Stellite156钴基合金涂层的作用机制[J].稀有金属与硬质合金,2021,49(4):29-34. 被引量:4

6马植甄,朱佳浩,张晖.Si对高熵合金涂层组织和高温抗氧化性能的影响[J].金属热处理,2021,46(8):46-50. 被引量:1

7陈明宣,马强,孟君晟,李成硕,史晓萍.高熵合金涂层的研究进展[J].金属热处理,2021,46(9):7-14. 被引量:4

8于克东,赵伟,张辉.离焦量对激光熔覆TiCoNiCrFe高熵合金涂层组织与性能的影响研究[J].齐鲁工业大学学报,2021,35(5):55-59. 被引量:2

9时海芳,王红蕾,李强,张正强,刘忆.B_(4)C对氩弧熔覆AlCuFeNiCo高熵合金涂层组织及性能的影响[J].材料保护,2021,54(11):27-30.

10商昭,白文芳,董潇婉,杨君刚.高熵合金特性和力学性能的研究进展[J].热加工工艺,2022,51(2):11-16. 被引量:3

1蒋烨,陈可,王伟.机械合金化法制备AlCoNiFeCr高熵合金涂层[J].中国有色金属学报,2018,28(9):1784-1790. 被引量:10

2周航,杨少锋,杨亚楠,严星,杨威,田华东.高熵合金的研究进展及发展趋势[J].热加工工艺,2018,47(18):5-9. 被引量:19

3董世知,孟旭,马壮,赵越超.粉煤灰活性氩弧熔覆Fe_xAlCoCrCuTi_(0.4)高熵合金涂层的组织和冲蚀磨损性能[J].材料保护,2018,51(8):90-94. 被引量:2

4面心立方单相高熵合金非金属夹杂物对力学性能的影响[J].金属功能材料,2018,25(5):62-62.

5向硕,张雷,刘学,乐国敏,戴晓军,李强,李晋锋.激光熔化沉积工艺对CrMnFeCoNi高熵合金组织和性能的影响[J].材料热处理学报,2018,39(10):29-35. 被引量:10

6AlxFeNiCrCo高熵合金[J].金属功能材料,2018,25(5):70-70.

7魏永生,王茂森,康健,马瑞欣,韦露,李建伟,赵新生.电沉积法制备三维泡沫镍负载钴催化剂及其工艺条件优化[J].材料导报,2018,32(19):3304-3308. 被引量:1

8王志刚.GH907合金铸锭均匀化热处理[J].中国冶金,2018,28(9):33-36. 被引量:3

9澹台凡亮,田洪芳,侯庆玲,郎坤,夏文波.现场激光增材修复风机转子轴实验及组织性能研究[J].热喷涂技术,2018,10(3):76-81. 被引量:1

10苗小锋,李正秋,汪云程.Si元素对CoCrAlY涂层组织及性能的影响[J].热喷涂技术,2018,10(3):23-26. 被引量:2

Basic Information:

DOI:

Chinese Library Classification Number:TG113[金属学及工艺—物理冶金]

Citation Information:

The (FeCrCo/Ni)5-SiTiNbMoW high-entropy alloy coatings were successfully prepared on the surface of the tool steel by laser cladding technology. The microstructure,composition, phase and hardness of the coatings were analyzed and tested by SEM/EDS, XRD and microhardness tester. The results show that the (FeCrCo)5-SiTiNbMoW coating contains BCC main phase,and a small amount of MC phase and Laves phase. The (FeCrNi)5-SiTiNbMoW coating contains FCC main phase and a small amount of MC phase and Laves phase. The two coatings are dominated by dendrites,while the (FeCrNi)5-SiTiNbMoW coating also has eutectic microstructure. The microhardness of the (FeCrCo)5-SiTiNbMoW high-entropy alloy coating is slightly higher than that of the (FeCrNi)5-SiTiNbMoW high-entropy alloy coating.

quote

GB/T 7714-2015 [1] WANG Yin, SHANG Xiao-juan, TIAN Xing-qiang, et al. Study on Microstructure and Properties of Laser Cladding(FeCrCo/Ni)_5-SiTiNbMoW High-entropy Alloy Coatings[J]. Rare Metals and Cemented Carbides, 2018(5): 30-36.
MLA [1] WANG Yin, et al., "Study on Microstructure and Properties of Laser Cladding(FeCrCo/Ni)_5-SiTiNbMoW High-entropy Alloy Coatings." Rare Metals and Cemented Carbides, no. 5, 2018, pp. 30-36.
APA [1] WANG Yin, SHANG Xiao-juan, TIAN Xing-qiang, GUO Ya-xiong, WANG Zhen, & CHEN Jia. (2018). Study on Microstructure and Properties of Laser Cladding(FeCrCo/Ni)_5-SiTiNbMoW High-entropy Alloy Coatings. Rare Metals and Cemented Carbides(5), 30-36.
IEEE [1] WANG Yin, SHANG Xiao-juan, TIAN Xing-qiang, GUO Ya-xiong, WANG Zhen, and CHEN Jia, "Study on Microstructure and Properties of Laser Cladding(FeCrCo/Ni)_5-SiTiNbMoW High-entropy Alloy Coatings," Rare Metals and Cemented Carbides, no. 5, pp. 30-36, 2018. keywords: {high entropy alloy;coating;laser cladding;microstructure;phase;hardness}