Rare Earth Superconducting Materials AITranslate

Hunan Provincial Science and Technology Commission
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Present paper briefly describes the properties of RE superconducting materials. forming process、 research and development, gives the achievements in Hunan RE superconducting materials aid some suggestions for their development.

KeyWords AITranslate

rare earth superconducting materials status suggestion.

1曹华茹,张云华,侯仰龙.稀土高新功能材料[J].化学教育,2000,15(4):1-5. 被引量:9

1谢建昌,李全安,李建弘,李克杰.稀土钇及其应用现状[J].稀有金属与硬质合金,2008,36(1):56-58. 被引量:18

2闫勇,朱伟长,李辉生.氧化钇纳米粉体材料的制备[J].化工新型材料,2004,32(7):11-12. 被引量:5

3朱伟长,钱元英,许盘凤.二氧化铈纳米粒子的制备[J].安徽工业大学学报:自然科学版,2004,21(4):282-284. 被引量:2

4李灵芝,李建渠.建立化学教学信息库,培养学生创新能力[J].科技信息,2007(32):224-224.

5李中华,朱伟长.氧化镝纳米粉体材料的制备[J].甘肃冶金,2013,35(6):56-57. 被引量:2

6李灵芝.利用最新科技信息,改进无机化学课堂教学[J].平顶山师专学报,2001,16(4):84-85.

7茅炜清,王绍武,陈耀峰.稀土元素在生产和生活中的应用[J].化学教育,2016,37(10):1-6. 被引量:8

8张诗曼,李存璞.基于科学态度与社会责任的反向思维教学——以“元素化学”为例[J].化学教育(中英文),2020,41(9):31-40. 被引量:3

9何玲,孙福海,徐琪鹏.电沉积法从废弃FCC催化剂中回收稀土元素的研究[J].现代化工,2021,41(5):108-113. 被引量:1

1德国马普学会利用激光照射技术开发稀土超导材料[J].企业技术开发,2011(4):187-187.

2陈东.德国利用激光技术研发稀土超导材料[J].功能材料信息,2011,8(2):50-50.

3德国马普学会利用激光照射技术开发稀土超导材料[J].大众科技,2011(4):9-9.

Basic Information:

DOI:

Chinese Library Classification Number:TM26[一般工业技术—材料科学与工程]

Citation Information:

Present paper briefly describes the properties of RE superconducting materials. forming process、 research and development, gives the achievements in Hunan RE superconducting materials aid some suggestions for their development.

quote

GB/T 7714-2015 [1] DING Bi-yun. Rare Earth Superconducting Materials[J]. Rare Metals and Cemented Carbides, 1994(3): 48-52.
MLA [1] DING Bi-yun. "Rare Earth Superconducting Materials." Rare Metals and Cemented Carbides, no. 3, 1994, pp. 48-52.
APA [1] DING Bi-yun. (1994). Rare Earth Superconducting Materials. Rare Metals and Cemented Carbides(3), 48-52.
IEEE [1] DING Bi-yun, "Rare Earth Superconducting Materials," Rare Metals and Cemented Carbides, no. 3, pp. 48-52, 1994. keywords: {rare earth superconducting materials, status, suggestion.}