Environmentally Friendly Methylcellulose Blend Binder for Hydrophobic Dust Control AITranslate

University of Arizona; University of Arizona; University of Arizona; University of Arizona
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A critical demand has existed for the past two decades to develop environmentally friendly, naturally degradable, and cost-effective materials to mitigate hydrophobic pollutants that directly endanger the environment and public health. Here, a newly developed methylcellulose blend (MCB), composed of hydroxypropyl methylcellulose (HPMC) and liquid amphiphilic polymer (LAP), synergistically enhanced the wettability of hydrophobic particles as a water additive and increased the average particle size as a binder. This observation was leveraged to evaluate MCB-based dust controlling materials via air filtering performance, mechanical vibration, and wind erosion tests. The filtration efficiency of filter membranes was enhanced up to 95% by a spray coating of MCB, while maintaining the same breathability as the untreated membrane. MCB sprayed on the surface of dust sources reduced generation of inhalable dust of <10 μm diameter up to 90% against a stream of air at 25 m/s compared to water treatment as a control. The effectiveness was maximal at 0.1% (w/v) HPMC and LAP due to molecular interactions between the MCB and hydrophobic dust at certain MCB constituent ratios. Altogether, the synergistic wettability and adhesiveness of the MCB provide the fundamental scientific concept and the technological progress to develop environmentally friendly formulations for advanced dust control technology.

KeyWords AITranslate

hydrophobic dust hydroxypropyl methylcellulose liquid amphiphilic polymer methylcellulose blend dust suppressant air filter
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01887

Chinese Library Classification Number:

Citation Information:

A critical demand has existed for the past two decades to develop environmentally friendly, naturally degradable, and cost-effective materials to mitigate hydrophobic pollutants that directly endanger the environment and public health. Here, a newly developed methylcellulose blend (MCB), composed of hydroxypropyl methylcellulose (HPMC) and liquid amphiphilic polymer (LAP), synergistically enhanced the wettability of hydrophobic particles as a water additive and increased the average particle size as a binder. This observation was leveraged to evaluate MCB-based dust controlling materials via air filtering performance, mechanical vibration, and wind erosion tests. The filtration efficiency of filter membranes was enhanced up to 95% by a spray coating of MCB, while maintaining the same breathability as the untreated membrane. MCB sprayed on the surface of dust sources reduced generation of inhalable dust of <10 μm diameter up to 90% against a stream of air at 25 m/s compared to water treatment as a control. The effectiveness was maximal at 0.1% (w/v) HPMC and LAP due to molecular interactions between the MCB and hydrophobic dust at certain MCB constituent ratios. Altogether, the synergistic wettability and adhesiveness of the MCB provide the fundamental scientific concept and the technological progress to develop environmentally friendly formulations for advanced dust control technology.

quote

GB/T 7714-2015 [1] Taehee Lee, Christopher P. Camp, Bumjoon Kim, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01887.
MLA [1] Taehee Lee, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01887.
APA [1] Taehee Lee, Christopher P. Camp, Bumjoon Kim, & Minkyu Kim. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01887
IEEE [1] Taehee Lee, Christopher P. Camp, Bumjoon Kim, and Minkyu Kim, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01887. keywords: {hydrophobic dust;hydroxypropyl methylcellulose;liquid amphiphilic polymer;methylcellulose blend;dust suppressant;air filter}