Bistacked Titanium Carbide (MXene) Anodes for Hybrid Sodium-Ion Capacitors AITranslate

Drexel University; Drexel University; Drexel University; Drexel University; King Abdullah University of Science and Technology (KAUST); Drexel University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Two-dimensional transition-metal carbides (MXenes) have shown great promise as electrode materials for high-rate pseudocapacitive energy storage. In this study, we report on the fabrication of bistacked two-dimensional titanium carbide electrodes which are free of binder, conductive additives, and current-collector. This MXene electrode is capable of reversible electrochemical storage of sodium ions with good cycling stability and rate capability. A prototype hybrid Na-ion capacitor was assembled by combining the bistacked MXene anode with an activated carbon cathode, which showed an energy density of 39 Wh/kg (including the total weight of bistacked MXene and activated carbon, 6 mg/cm2) at 1C rate and maintained up to 60% of its performance at a 60C rate, in the operating voltage window of 3.4 V. This study opens new avenues for developing self-standing binder and additive-free MXene electrodes for metal-ion batteries and capacitors.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b01062

Chinese Library Classification Number:

Citation Information:

Two-dimensional transition-metal carbides (MXenes) have shown great promise as electrode materials for high-rate pseudocapacitive energy storage. In this study, we report on the fabrication of bistacked two-dimensional titanium carbide electrodes which are free of binder, conductive additives, and current-collector. This MXene electrode is capable of reversible electrochemical storage of sodium ions with good cycling stability and rate capability. A prototype hybrid Na-ion capacitor was assembled by combining the bistacked MXene anode with an activated carbon cathode, which showed an energy density of 39 Wh/kg (including the total weight of bistacked MXene and activated carbon, 6 mg/cm2) at 1C rate and maintained up to 60% of its performance at a 60C rate, in the operating voltage window of 3.4 V. This study opens new avenues for developing self-standing binder and additive-free MXene electrodes for metal-ion batteries and capacitors.

quote

GB/T 7714-2015 [1] Narendra Kurra, Mohamed Alhabeb, Kathleen Maleski, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b01062.
MLA [1] Narendra Kurra, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b01062.
APA [1] Narendra Kurra, Mohamed Alhabeb, Kathleen Maleski, ChuehHan Wang, Husam N. Alshareef, & Yury Gogotsi. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b01062
IEEE [1] Narendra Kurra, Mohamed Alhabeb, Kathleen Maleski, ChuehHan Wang, Husam N. Alshareef, and Yury Gogotsi, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b01062.