Effect of variable material properties and environmental conditions on thermomechanical phase transformations in shape memory alloy wires AITranslate

2801 South University; 2801 South University; 2801 South University
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

This paper reports a computational study of the impact of variable material properties and environmental conditions (thermal boundary conditions and convection coefficients) on shape memory alloy wires undergoing (i) zero-stress, thermally-induced phase transformations, and (ii) stress-induced phase transformations at constant stress rates. A finite difference numerical approach has been employed, and has been validated by comparing with two analytical solutions. The results have been all given in non-dimensional form, and within the context of the range of parameters that have been studied, the following recommendations can be made for shape memory alloys (SMA) actuator design: (i) an uncertainty in the thermal boundary condition is not as important as long as the design process allows for a full transformation back to martensite at the end of a cycle of martensite–austenite–martensite thermal transformation, (ii) uncertainties in the thermal boundary condition, convection coefficient and thermal material properties are not as important when the phase transformation in a SMA is induced by stress.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/S0927-0256(03)00049-1

Chinese Library Classification Number:

Citation Information:

This paper reports a computational study of the impact of variable material properties and environmental conditions (thermal boundary conditions and convection coefficients) on shape memory alloy wires undergoing (i) zero-stress, thermally-induced phase transformations, and (ii) stress-induced phase transformations at constant stress rates. A finite difference numerical approach has been employed, and has been validated by comparing with two analytical solutions. The results have been all given in non-dimensional form, and within the context of the range of parameters that have been studied, the following recommendations can be made for shape memory alloys (SMA) actuator design: (i) an uncertainty in the thermal boundary condition is not as important as long as the design process allows for a full transformation back to martensite at the end of a cycle of martensite–austenite–martensite thermal transformation, (ii) uncertainties in the thermal boundary condition, convection coefficient and thermal material properties are not as important when the phase transformation in a SMA is induced by stress.

quote

GB/T 7714-2015 [1] K Sadek, A Bhattacharyya, W Moussa. Computational Materials Science, 2003(27). DOI:10.1016/S0927-0256(03)00049-1.
MLA [1] K Sadek, et al., Computational Materials Science, no. 27, 2003, https://doi.org/10.1016/S0927-0256(03)00049-1.
APA [1] K Sadek, A Bhattacharyya, & W Moussa. (2003). Computational Materials Science(27). https://doi.org/10.1016/S0927-0256(03)00049-1
IEEE [1] K Sadek, A Bhattacharyya, and W Moussa, Computational Materials Science, no. 27, 2003, doi: 10.1016/S0927-0256(03)00049-1.