Realizing High-Detectivity Near-Infrared Photodetectors in Tin–Lead Perovskites by Double-Sided Surface-Preferred Distribution of Multifunctional Tin Thiocyanate Additive AITranslate

The University of Hong Kong; Sun Yat-sen University; The University of Hong Kong; The University of Hong Kong; The Hong Kong Polytechnic University; The Hong Kong University of Science and Technology; The University of Hong Kong
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Tin–lead perovskite photodetectors are attractive alternatives to silicon counterparts for near-infrared photodetection, due to their outstanding optoelectronic properties, solution processability, and flexible compatibility. However, uncontrollable crystallization and easy oxidation problems of tin-containing perovskites severely hinder advances in their perfomance. Herein, we develop a high-detectivity near-infrared photodetector using a tailored tin-lead perovskite structure. Notably, we employ tin thiocyanate to form a double-sided surface-preferred distribution in tin-lead perovskites, in which the majority is located at bottom and top surfaces, and the tiny minority positioned inside the films. The tailored perovskite structure with the unique additive distribution significantly improves the film morphology and antioxidation ability. Finally, self-powered tin-lead perovskite photodetectors achieve a peak responsivity of 0.57 A W–1, a detectivity of 8.48 × 1012 Jones at 910 nm, and a large linear dynamic range of 213 dB, accompanied by an outstanding lifetime of 2300 h. This work opens up a new avenue to developing high-performance near-infrared photodetectors.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.2c02055

Chinese Library Classification Number:

Citation Information:

Tin–lead perovskite photodetectors are attractive alternatives to silicon counterparts for near-infrared photodetection, due to their outstanding optoelectronic properties, solution processability, and flexible compatibility. However, uncontrollable crystallization and easy oxidation problems of tin-containing perovskites severely hinder advances in their perfomance. Herein, we develop a high-detectivity near-infrared photodetector using a tailored tin-lead perovskite structure. Notably, we employ tin thiocyanate to form a double-sided surface-preferred distribution in tin-lead perovskites, in which the majority is located at bottom and top surfaces, and the tiny minority positioned inside the films. The tailored perovskite structure with the unique additive distribution significantly improves the film morphology and antioxidation ability. Finally, self-powered tin-lead perovskite photodetectors achieve a peak responsivity of 0.57 A W–1, a detectivity of 8.48 × 1012 Jones at 910 nm, and a large linear dynamic range of 213 dB, accompanied by an outstanding lifetime of 2300 h. This work opens up a new avenue to developing high-performance near-infrared photodetectors.

quote

GB/T 7714-2015 [1] Hui Liu, Lu Zhu, Hong Zhang, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.2c02055.
MLA [1] Hui Liu, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.2c02055.
APA [1] Hui Liu, Lu Zhu, Hong Zhang, Xinjun He, Feng Yan, Kam Sing Wong, & Wallace C. H. Choy. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.2c02055
IEEE [1] Hui Liu, Lu Zhu, Hong Zhang, Xinjun He, Feng Yan, Kam Sing Wong, and Wallace C. H. Choy, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.2c02055.