Soft Actuators Enabled by 3D-Architected Low Melting Point Alloys/Polymer Composites with a Large Switching Range AITranslate
Abstract AITranslate
Materials with switchable stiffness, especially dynamically switchable stiffness with a large switching range, have aroused considerable interest in the field of soft actuators. Herein, we designed a three-dimensional (3D)-architected Field’s metal (FM) microstructure and embedded it into a kind of designed phase-changing side-chain stiffness variable polymer to obtain a composite (SUFM) with superior stiffness switchable capacity. SUFM exhibits excellent conductivity under low volume fraction (31.5%). What is more, owing to the rapid solid–liquid switch and ultra-high modulus of FM, the rigid/soft stiffness switch ratio of SUFM can reach up to ultra-high 7532-folds. In addition to the superior stiffness switchable capacity, SUFM also exhibits outstanding shape memory and self-healing properties. Subsequently, a SUFM film was attached to a kind of designed 3D-printing fast-response and stiffness-tunable soft actuator as the stiffness variable unit. The soft actuator has a fast heating–cooling cycle of 41 s under 10 A current with 4 °C water as a coolant. Besides, the stiffness and net force of the soft actuator can reach up to 944 mN/mm and 4590 mN, respectively. The high load capacity and superior switchable stiffness are demonstrated by a robotic gripper equipped with three assembled soft actuators on a 3D-printing base, which can lift objects of arbitrary shapes and various weights up to 2 kg. This work may be further developed into smart components that can be widely used in soft actuators.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c01048
Chinese Library Classification Number:
Citation Information:
Materials with switchable stiffness, especially dynamically switchable stiffness with a large switching range, have aroused considerable interest in the field of soft actuators. Herein, we designed a three-dimensional (3D)-architected Field’s metal (FM) microstructure and embedded it into a kind of designed phase-changing side-chain stiffness variable polymer to obtain a composite (SUFM) with superior stiffness switchable capacity. SUFM exhibits excellent conductivity under low volume fraction (31.5%). What is more, owing to the rapid solid–liquid switch and ultra-high modulus of FM, the rigid/soft stiffness switch ratio of SUFM can reach up to ultra-high 7532-folds. In addition to the superior stiffness switchable capacity, SUFM also exhibits outstanding shape memory and self-healing properties. Subsequently, a SUFM film was attached to a kind of designed 3D-printing fast-response and stiffness-tunable soft actuator as the stiffness variable unit. The soft actuator has a fast heating–cooling cycle of 41 s under 10 A current with 4 °C water as a coolant. Besides, the stiffness and net force of the soft actuator can reach up to 944 mN/mm and 4590 mN, respectively. The high load capacity and superior switchable stiffness are demonstrated by a robotic gripper equipped with three assembled soft actuators on a 3D-printing base, which can lift objects of arbitrary shapes and various weights up to 2 kg. This work may be further developed into smart components that can be widely used in soft actuators.
quote
| GB/T 7714-2015 | [1] Yahao Liu, Yuansheng Wang, Xue Yang, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01048. |
| MLA | [1] Yahao Liu, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01048. |
| APA | [1] Yahao Liu, Yuansheng Wang, Xue Yang, Jian Zheng, Wei Huang, Yu Zhang, Xiao Zhang, & Xuan Wang. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01048 |
| IEEE | [1] Yahao Liu, Yuansheng Wang, Xue Yang, Jian Zheng, Wei Huang, Yu Zhang, Xiao Zhang, and Xuan Wang, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01048. keywords: {stiffness switchable;phase changing;shape memory;soft actuator;Field’s metal} |