Sulfur-Doped Defective Nanocarbons Derived from Fullerenes as Electrocatalysts for Efficient and Selective H2O2 Electroproduction AITranslate

Hefei University of Technology; Huazhong University of Science and Technology; Hefei University of Technology; Hefei University of Technology; Hebei University of Engineering; Princess Nourah bint Abdulrahman University; Hefei University of Technology; Hefei University of Technology; Huazhong University of Science and Technology; Huazhong University of Science and Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Carbon nanomaterials have shown attractive application prospects for efficient electrocatalysis for two-electron oxygen reduction reaction (2e– ORR) toward hydrogen peroxide (H2O2) electroproduction. By synthesizing sulfur-doped defective nanocarbons (S-DNC) through direct pyrolysis in the presence of sulfur, utilizing fullerene (C60) as the precursor, we achieved promising results. The as-obtained S-DNC catalyst demonstrated a high ORR onset potential of 0.78 V and high selectivity toward the 2e– pathway (∼90%). Importantly, when used as the cathode catalyst in a H cell, the S-DNC electrode exhibited impressive features such as a high H2O2 yield rate (690 mg L–1 h–1), quantitative faradic efficiency (∼100%), and rapid organic pollutant degradation rate. Theoretical calculations revealed that the combination of pentagon defects and sulfur dopants synergistically promoted the activation of the O2 molecule and facilitated the desorption of oxygen intermediates. This discovery significantly contributes to the understanding and advancement of carbon-based catalysts for efficient electroproduction of H2O2 by incorporating heteroatom dopants and topological pentagon defects synergistically.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.3c01036

Chinese Library Classification Number:

Citation Information:

Carbon nanomaterials have shown attractive application prospects for efficient electrocatalysis for two-electron oxygen reduction reaction (2e– ORR) toward hydrogen peroxide (H2O2) electroproduction. By synthesizing sulfur-doped defective nanocarbons (S-DNC) through direct pyrolysis in the presence of sulfur, utilizing fullerene (C60) as the precursor, we achieved promising results. The as-obtained S-DNC catalyst demonstrated a high ORR onset potential of 0.78 V and high selectivity toward the 2e– pathway (∼90%). Importantly, when used as the cathode catalyst in a H cell, the S-DNC electrode exhibited impressive features such as a high H2O2 yield rate (690 mg L–1 h–1), quantitative faradic efficiency (∼100%), and rapid organic pollutant degradation rate. Theoretical calculations revealed that the combination of pentagon defects and sulfur dopants synergistically promoted the activation of the O2 molecule and facilitated the desorption of oxygen intermediates. This discovery significantly contributes to the understanding and advancement of carbon-based catalysts for efficient electroproduction of H2O2 by incorporating heteroatom dopants and topological pentagon defects synergistically.

quote

GB/T 7714-2015 [1] Wangqiang Shen, Chang Zhang, Xinyu Wang, et al. ACS Materials Letters, 2024(6). DOI:10.1021/acsmaterialslett.3c01036.
MLA [1] Wangqiang Shen, et al., ACS Materials Letters, no. 6, 2024, https://doi.org/10.1021/acsmaterialslett.3c01036.
APA [1] Wangqiang Shen, Chang Zhang, Xinyu Wang, Yuzhong Huang, Zhiling Du, Muneerah Alomar, Junjie Wang, Jun Lv, Jian Zhang, & Xing Lu. (2024). ACS Materials Letters(6). https://doi.org/10.1021/acsmaterialslett.3c01036
IEEE [1] Wangqiang Shen, Chang Zhang, Xinyu Wang, Yuzhong Huang, Zhiling Du, Muneerah Alomar, Junjie Wang, Jun Lv, Jian Zhang, and Xing Lu, ACS Materials Letters, no. 6, 2024, doi: 10.1021/acsmaterialslett.3c01036.