daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Ultrastrong and flame-resistant freestanding films from nanocelluloses, self-assembled using a layer-by-layer approach AITranslate

KTH Royal Institute of Technology;Dipartimento di Scienza Applicata e Technologia, Politecnico di Torino; KTH Royal Institute of Technology
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Nanosized cellulose nanofibrils (CNF) prepared from phosphorylated pulp fibers (P-CNF) are combined with CNF prepared from aminated fibers (cationic CNF) through a layer-by-layer (LbL) assembly to prepare a freestanding, transparent all-cellulose film. It is shown that the thermal stability and flame-retardant properties of the all CNF film are significantly improved when phosphorylated CNF is combined with cationic fibrils in an LbL assembled structure. The freestanding films also show a tensile strength of 160 MPa and a Young`s modulus of 9 GPa, placing it among strongest freestanding LbL films fabricated so far, showing large promise for the use of these types of ultrathin films in advanced applications. The LbL build-up of the cationic CNF/P-CNF multilayer film is carefully studied by quartz crystal microbalance with dissipation (QCM-D) and atomic force microscopy (AFM). Hydrophobized silicon substrates are used for the LbL deposition and it is shown that the (cationic CNF/P-CNF)300 film, 2.3 μm thick, can be easily detached from the substrate using tweezers. The thermal stability, combustion behavior and mechanical properties of the films are further studied by thermogravimetric analysis, combustion and tensile tests respectively. Graphical abstract Download : Download high-res image (144KB) Download : Download full-size image

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.apmt.2017.08.002

Chinese Library Classification Number:

Citation Information:

Nanosized cellulose nanofibrils (CNF) prepared from phosphorylated pulp fibers (P-CNF) are combined with CNF prepared from aminated fibers (cationic CNF) through a layer-by-layer (LbL) assembly to prepare a freestanding, transparent all-cellulose film. It is shown that the thermal stability and flame-retardant properties of the all CNF film are significantly improved when phosphorylated CNF is combined with cationic fibrils in an LbL assembled structure. The freestanding films also show a tensile strength of 160 MPa and a Young`s modulus of 9 GPa, placing it among strongest freestanding LbL films fabricated so far, showing large promise for the use of these types of ultrathin films in advanced applications. The LbL build-up of the cationic CNF/P-CNF multilayer film is carefully studied by quartz crystal microbalance with dissipation (QCM-D) and atomic force microscopy (AFM). Hydrophobized silicon substrates are used for the LbL deposition and it is shown that the (cationic CNF/P-CNF)300 film, 2.3 μm thick, can be easily detached from the substrate using tweezers. The thermal stability, combustion behavior and mechanical properties of the films are further studied by thermogravimetric analysis, combustion and tensile tests respectively. Graphical abstract Download : Download high-res image (144KB) Download : Download full-size image

quote

GB/T 7714-2015 [1] Maryam Ghanadpour, Federico Carosio, Lars Wågberg. Applied Materials Today, 2017(9). DOI:10.1016/j.apmt.2017.08.002.
MLA [1] Maryam Ghanadpour, et al., Applied Materials Today, no. 9, 2017, https://doi.org/10.1016/j.apmt.2017.08.002.
APA [1] Maryam Ghanadpour, Federico Carosio, & Lars Wågberg. (2017). Applied Materials Today(9). https://doi.org/10.1016/j.apmt.2017.08.002
IEEE [1] Maryam Ghanadpour, Federico Carosio, and Lars Wågberg, Applied Materials Today, no. 9, 2017, doi: 10.1016/j.apmt.2017.08.002.