Abstract AITranslate

Determining the molecular orientation at the single molecule level is of key importance for a wide range of applications ranging from molecular electronic devices to biomedical applications. In this work surface-enhanced Raman scattering (SERS) was used to probe the light-emitting conjugated polymer F8-PFB at the single molecule level using nanoparticles on an extended metallic film nanogap. The directional field enhancement of the nanogap combined with density functional theory (DFT) calculations was used to determine the orientation of the molecule. This analysis revealed that the spin-coated conjugated polymer preferentially aligns its molecular chains parallel to the metallic substrate. The integration of this approach in nanofabrication and synthesis will have a profound impact on different fields ranging from molecular electronic devices to biomedical applications.

KeyWords AITranslate

Raman SERS conjugated polymer DFT nanogap
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00180

Chinese Library Classification Number:

Citation Information:

Determining the molecular orientation at the single molecule level is of key importance for a wide range of applications ranging from molecular electronic devices to biomedical applications. In this work surface-enhanced Raman scattering (SERS) was used to probe the light-emitting conjugated polymer F8-PFB at the single molecule level using nanoparticles on an extended metallic film nanogap. The directional field enhancement of the nanogap combined with density functional theory (DFT) calculations was used to determine the orientation of the molecule. This analysis revealed that the spin-coated conjugated polymer preferentially aligns its molecular chains parallel to the metallic substrate. The integration of this approach in nanofabrication and synthesis will have a profound impact on different fields ranging from molecular electronic devices to biomedical applications.

quote

GB/T 7714-2015 [1] Addison R. L. Marshall, Matthew Roberts, Johannes Gierschner, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00180.
MLA [1] Addison R. L. Marshall, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00180.
APA [1] Addison R. L. Marshall, Matthew Roberts, Johannes Gierschner, JeanSebastien G. Bouillard, & Ali M. Adawi. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00180
IEEE [1] Addison R. L. Marshall, Matthew Roberts, Johannes Gierschner, JeanSebastien G. Bouillard, and Ali M. Adawi, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00180. keywords: {Raman;SERS;conjugated polymer;DFT;nanogap}