Facilitating Lithium-Ion Conduction in Gel Polymer Electrolyte by Metal-Organic Frameworks AITranslate

Department of Chemical and Biomolecular Engineering University of California;Department of Chemical and Biomolecular Engineering University of California;Department of Chemical and Biomolecular Engineering University of California;Department of Chemical and Biomolecular Engineering University of California;Department of Chemical and Biomolecular Engineering University of California;Department of Chemical and Biomolecular Engineering University of California
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Gel polymer electrolytes (GPL) that comprise polymer, lithium salts, and organic plasticizers hold great promise for safer lithium-ion batteries, because of liquid-like ionic conductivity, as well as solid-like leakage-free property. However, only a small portion of ion conduction effectively carried by Li+ ions (or low Li+ transference number) gives rise to poor interfacial stability between GPL with electrodes and limited practicability. Here, metal-organic framework (MOF) containing open-metal sites (OMSs) are used as fillers that endow GPL simultaneously with high ionic conductivity (>1 mS cm–1) and a high Li+ transference number (up to 0.66), which results from immobilized anions and facilitated cation conduction by virtue of OMSs. Implementations of the GPL with OMSs-laden MOF in pseudo-solid-state batteries afford affinitive interfaces involving metallic Li and intercalation-type electrodes (LiFePO4, Li4Ti5O12), which contribute to significant improvements in battery durability and thereby could introduce a new type of MOF fillers for solid-state polymer electrolytes.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.0c00293

Chinese Library Classification Number:

Citation Information:

Gel polymer electrolytes (GPL) that comprise polymer, lithium salts, and organic plasticizers hold great promise for safer lithium-ion batteries, because of liquid-like ionic conductivity, as well as solid-like leakage-free property. However, only a small portion of ion conduction effectively carried by Li+ ions (or low Li+ transference number) gives rise to poor interfacial stability between GPL with electrodes and limited practicability. Here, metal-organic framework (MOF) containing open-metal sites (OMSs) are used as fillers that endow GPL simultaneously with high ionic conductivity (>1 mS cm–1) and a high Li+ transference number (up to 0.66), which results from immobilized anions and facilitated cation conduction by virtue of OMSs. Implementations of the GPL with OMSs-laden MOF in pseudo-solid-state batteries afford affinitive interfaces involving metallic Li and intercalation-type electrodes (LiFePO4, Li4Ti5O12), which contribute to significant improvements in battery durability and thereby could introduce a new type of MOF fillers for solid-state polymer electrolytes.

quote

GB/T 7714-2015 [1] Xing Lu, Haiping Wu, Dejia Kong, et al. ACS Materials Letters, 2020(2). DOI:10.1021/acsmaterialslett.0c00293.
MLA [1] Xing Lu, et al., ACS Materials Letters, no. 2, 2020, https://doi.org/10.1021/acsmaterialslett.0c00293.
APA [1] Xing Lu, Haiping Wu, Dejia Kong, Xinru Li, Li Shen, & Yunfeng Lu. (2020). ACS Materials Letters(2). https://doi.org/10.1021/acsmaterialslett.0c00293
IEEE [1] Xing Lu, Haiping Wu, Dejia Kong, Xinru Li, Li Shen, and Yunfeng Lu, ACS Materials Letters, no. 2, 2020, doi: 10.1021/acsmaterialslett.0c00293.