Decorating soft electrified interfaces: From molecular assemblies to nano-objects AITranslate
Abstract AITranslate
The interface formed between two immiscible electrolyte solutions (ITIES) constitutes a fantastic playground for the investigation of charge (under the form of either ion or electron) transfer processes. We have reviewed here the routes for the modification of such soft interfaces by an accurate electrochemical control. The three main strategies developed in the past four decades include (i) the electrochemically controlled assembly of molecules and nano-objects; (ii) the in situ electrogeneration of nanomaterials and (iii) the use of ex situ synthesized membranes. Applications of functionalized ITIES in the fields of redox catalysis and electroanalysis of modified soft interfaces are also discussed. Graphical abstract Download : Download high-res image (146KB) Download : Download full-size image
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.apmt.2017.10.001
Chinese Library Classification Number:
Citation Information:
The interface formed between two immiscible electrolyte solutions (ITIES) constitutes a fantastic playground for the investigation of charge (under the form of either ion or electron) transfer processes. We have reviewed here the routes for the modification of such soft interfaces by an accurate electrochemical control. The three main strategies developed in the past four decades include (i) the electrochemically controlled assembly of molecules and nano-objects; (ii) the in situ electrogeneration of nanomaterials and (iii) the use of ex situ synthesized membranes. Applications of functionalized ITIES in the fields of redox catalysis and electroanalysis of modified soft interfaces are also discussed. Graphical abstract Download : Download high-res image (146KB) Download : Download full-size image
quote
| GB/T 7714-2015 | [1] Lukasz Poltorak, Alonso GameroQuijano, Grégoire Herzog, et al. Applied Materials Today, 2017(9). DOI:10.1016/j.apmt.2017.10.001. |
| MLA | [1] Lukasz Poltorak, et al., Applied Materials Today, no. 9, 2017, https://doi.org/10.1016/j.apmt.2017.10.001. |
| APA | [1] Lukasz Poltorak, Alonso GameroQuijano, Grégoire Herzog, & Alain Walcarius. (2017). Applied Materials Today(9). https://doi.org/10.1016/j.apmt.2017.10.001 |
| IEEE | [1] Lukasz Poltorak, Alonso GameroQuijano, Grégoire Herzog, and Alain Walcarius, Applied Materials Today, no. 9, 2017, doi: 10.1016/j.apmt.2017.10.001. |