daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Tröger’s Base-Cored Triarylamine Polyamide for Electrochromic Response Capability Enhancement AITranslate

National Taiwan University; National Taiwan University; National Taiwan University; National Taiwan University of Science and Technology; National Taiwan University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Recently, more and more researchers have focused on generating “pores” within the polymer matrix to prompt the performance of electrochromic (EC) films using physical or chemical approaches. In this work, we meticulously designed a Tröger’s base (TB)-cored arylamine-containing diamine monomer, TBTPA-NH2, and synthesized the corresponding redox-active polyamide, PTBTPA. The resulting PTBTPA exhibits low density with large d-spacing and surface area, contributing to the rigid and V-shaped TB unit. Consequently, the prepared polymer film demonstrated remarkable electrochemical and EC behaviors, such as low applied potential (1.00 V), facilitating rapid diffusion of the electrolyte, reasonable switching capability (1.8 s/1.5 s for coloring tc and bleaching tb, respectively), and excellent stability. For further application, the electrochromic device (ECD) of PTBTPA/HV exhibits the best-enhanced response capability (3.5 s/6.1 s for tc and tb, respectively), the highest coloration efficiency (337 cm2/C), and switching stability (96.1% of retention after 500-cycle switching).

KeyWords AITranslate

electrochromism quick response capability intrinsic microporosity Tröger’s base triarylamine
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c02288

Chinese Library Classification Number:

Citation Information:

Recently, more and more researchers have focused on generating “pores” within the polymer matrix to prompt the performance of electrochromic (EC) films using physical or chemical approaches. In this work, we meticulously designed a Tröger’s base (TB)-cored arylamine-containing diamine monomer, TBTPA-NH2, and synthesized the corresponding redox-active polyamide, PTBTPA. The resulting PTBTPA exhibits low density with large d-spacing and surface area, contributing to the rigid and V-shaped TB unit. Consequently, the prepared polymer film demonstrated remarkable electrochemical and EC behaviors, such as low applied potential (1.00 V), facilitating rapid diffusion of the electrolyte, reasonable switching capability (1.8 s/1.5 s for coloring tc and bleaching tb, respectively), and excellent stability. For further application, the electrochromic device (ECD) of PTBTPA/HV exhibits the best-enhanced response capability (3.5 s/6.1 s for tc and tb, respectively), the highest coloration efficiency (337 cm2/C), and switching stability (96.1% of retention after 500-cycle switching).

quote

GB/T 7714-2015 [1] MinHsiu Tu, YuJen Shao, HouLin Li, et al. ACS Applied Polymer Materials, 2024(6). DOI:10.1021/acsapm.3c02288.
MLA [1] MinHsiu Tu, et al., ACS Applied Polymer Materials, no. 6, 2024, https://doi.org/10.1021/acsapm.3c02288.
APA [1] MinHsiu Tu, YuJen Shao, HouLin Li, ChienChieh Hu, & GueySheng Liou. (2024). ACS Applied Polymer Materials(6). https://doi.org/10.1021/acsapm.3c02288
IEEE [1] MinHsiu Tu, YuJen Shao, HouLin Li, ChienChieh Hu, and GueySheng Liou, ACS Applied Polymer Materials, no. 6, 2024, doi: 10.1021/acsapm.3c02288. keywords: {electrochromism;quick response capability;intrinsic microporosity;Tröger’s base;triarylamine}