Bio-Inspired Structural Colors Based on Linear Ultrahigh Molecular Weight Block Copolymers AITranslate

Ernst-Berl-Institue for Chemical Engineering and Macromolecular Chemistry, Technische Universität Darmstadt;Ernst-Berl-Institue for Chemical Engineering and Macromolecular Chemistry, Technische Universität Darmstadt
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Ultrahigh molecular weight (UHMW) block copolymers (BCPs) are promising candidates for the fabrication of photonic materials. Here, we demonstrate the synthesis and self-assembly capability of well-defined amphiphilic UHMW BCPs with overall molar masses up to 4432 kg mol–1 obtained via living anionic polymerization. BCP micelles featuring hydrodynamic diameters in the range of the wavelength of the visible light to the near-infrared region (300–1143 nm) are used for colloidal crystal formation. By varying the BCP composition, brilliant structural colors can be observed. Microphase separation of the UHMW BCPs in the bulk state reveals uniform domains and showing blue to green structural color transitions. Finally, we provide examples of how BCP structural control can be used to generate reversibly switchable solvatochromatic optical sensors.

KeyWords AITranslate

anionic polymerization block copolymers selfassembly morphology photonic materials micellar photonic crystals Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.8b00169

Chinese Library Classification Number:

Citation Information:

Ultrahigh molecular weight (UHMW) block copolymers (BCPs) are promising candidates for the fabrication of photonic materials. Here, we demonstrate the synthesis and self-assembly capability of well-defined amphiphilic UHMW BCPs with overall molar masses up to 4432 kg mol–1 obtained via living anionic polymerization. BCP micelles featuring hydrodynamic diameters in the range of the wavelength of the visible light to the near-infrared region (300–1143 nm) are used for colloidal crystal formation. By varying the BCP composition, brilliant structural colors can be observed. Microphase separation of the UHMW BCPs in the bulk state reveals uniform domains and showing blue to green structural color transitions. Finally, we provide examples of how BCP structural control can be used to generate reversibly switchable solvatochromatic optical sensors.

quote

GB/T 7714-2015 [1] Michael Appold, Markus Gallei. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.8b00169.
MLA [1] Michael Appold, and Markus Gallei. ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.8b00169.
APA [1] Michael Appold, & Markus Gallei. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.8b00169
IEEE [1] Michael Appold and Markus Gallei, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.8b00169. keywords: {anionic polymerization;block copolymers;selfassembly;morphology;photonic materials;micellar photonic crystals;Show More}