High Conductivity and Durability Textile Gas Sensor-Based Polyaniline-Decorated-Poly(3,4-ethylenedioxythiophene)/Poly(4-styrenesulfonate) for Ammonia Detection AITranslate

Thammasat University; Kasetsart University; Mahidol University; Mahidol University; Sungkyunkwan University; Thammasat University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Securing the stability of sensing responses under stretching and washing is essential for textile-based wearable gas sensors. Herein, we report textile-based gas sensors composed of polyaniline (PANi)-decorated poly(3,4-ethylenedioxythiophene)/poly(4-styrenesulfonate) (PEDOT/PSS) coated on cotton yarn. Without conventional hydrochloric acid (HCl) doping, the PANi/PEDOT/PSS sensor exhibits a high electrical conductivity of 1343 S cm–1, good sensitivity, and excellent stability for detecting ammonia, obviously better than the PEDOT/PSS and PANi/HCl sensors. The ammonia sensing response of the PANi/PEDOT/PSS sensor was 7.54% (at 50 ppm), with a detection limit as low as 5 ppm. The enhanced sensing performance is attributed to the heterostructure of PANi and PEDOT/PSS films and the protonation/deprotonation nature of PANi. It was found that the sensing performance of the PANi/PEDOT/PSS sensor is humidity independent. More importantly, the sensor conductivity and sensing response have shown excellent stability under 1100 stretching/releasing cycles and high durability after 10 washing cycles. The results indicate a potential application of wearable textile sensors for detecting ammonia in an environment.

KeyWords AITranslate

electronic textile ammonia sensor PANi PEDOT/PSS washable
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01374

Chinese Library Classification Number:

Citation Information:

Securing the stability of sensing responses under stretching and washing is essential for textile-based wearable gas sensors. Herein, we report textile-based gas sensors composed of polyaniline (PANi)-decorated poly(3,4-ethylenedioxythiophene)/poly(4-styrenesulfonate) (PEDOT/PSS) coated on cotton yarn. Without conventional hydrochloric acid (HCl) doping, the PANi/PEDOT/PSS sensor exhibits a high electrical conductivity of 1343 S cm–1, good sensitivity, and excellent stability for detecting ammonia, obviously better than the PEDOT/PSS and PANi/HCl sensors. The ammonia sensing response of the PANi/PEDOT/PSS sensor was 7.54% (at 50 ppm), with a detection limit as low as 5 ppm. The enhanced sensing performance is attributed to the heterostructure of PANi and PEDOT/PSS films and the protonation/deprotonation nature of PANi. It was found that the sensing performance of the PANi/PEDOT/PSS sensor is humidity independent. More importantly, the sensor conductivity and sensing response have shown excellent stability under 1100 stretching/releasing cycles and high durability after 10 washing cycles. The results indicate a potential application of wearable textile sensors for detecting ammonia in an environment.

quote

GB/T 7714-2015 [1] Kuntima Pattanarat, Nattasamon Petchsang, Tanakorn Osotchan, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c01374.
MLA [1] Kuntima Pattanarat, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c01374.
APA [1] Kuntima Pattanarat, Nattasamon Petchsang, Tanakorn Osotchan, IMing Tang, YongHoon Kim, & Rawat Jaisutti. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c01374
IEEE [1] Kuntima Pattanarat, Nattasamon Petchsang, Tanakorn Osotchan, IMing Tang, YongHoon Kim, and Rawat Jaisutti, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c01374. keywords: {electronic textile;ammonia sensor;PANi;PEDOT/PSS;washable}