daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Aggregation-Induced Emission of a Two-Dimensional Covalent Organic Framework for Molecular Recognition in Quantitative Metrics AITranslate

Zhejiang University of Technology; Zhejiang University of Technology; Yancheng Teachers University; Yancheng Teachers University; Yancheng Teachers University; Zhejiang University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Fluorescent porous materials have been intensively examined owing to their versatile applications in molecular recognition and chemical sensing. Although many studies on luminescent two-dimensional (2D) covalent organic frameworks (COFs) for chemical sensing applications have been reported, precise linear control of the aggregation-induced luminescence effects in 2D COFs has been rarely achieved. Hereby, a highly crystalline 2D COF material bearing a tetraphenylethylene (TPE) molecule as a molecular rotor with a responsive fluorescence behavior is reported. Due to the varying extent of motion regulation of the TPE rotor with different volatile organic compounds (VOCs), the as-obtained fluorescent 2D COFs exhibit excellent sensitivity and selectivity in the qualitative and quantitative analysis of volatile organic compounds (VOCs). Notably, the fluorescence intensity derived from the aggregation-induced emission (AIE) is in a linear relationship with VOCs across a wide concentration range (0–3.0 × 103 mM), indicating their potential as effective VOC detectors.

KeyWords AITranslate

covalent organic frameworks aggregationinduced emission molecular rotor volatile organic compounds chemical sensing
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00388

Chinese Library Classification Number:

Citation Information:

Fluorescent porous materials have been intensively examined owing to their versatile applications in molecular recognition and chemical sensing. Although many studies on luminescent two-dimensional (2D) covalent organic frameworks (COFs) for chemical sensing applications have been reported, precise linear control of the aggregation-induced luminescence effects in 2D COFs has been rarely achieved. Hereby, a highly crystalline 2D COF material bearing a tetraphenylethylene (TPE) molecule as a molecular rotor with a responsive fluorescence behavior is reported. Due to the varying extent of motion regulation of the TPE rotor with different volatile organic compounds (VOCs), the as-obtained fluorescent 2D COFs exhibit excellent sensitivity and selectivity in the qualitative and quantitative analysis of volatile organic compounds (VOCs). Notably, the fluorescence intensity derived from the aggregation-induced emission (AIE) is in a linear relationship with VOCs across a wide concentration range (0–3.0 × 103 mM), indicating their potential as effective VOC detectors.

quote

GB/T 7714-2015 [1] Peng Jin, Chenglong Guo, Jiahao Li, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00388.
MLA [1] Peng Jin, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00388.
APA [1] Peng Jin, Chenglong Guo, Jiahao Li, Dejun Zhou, Guodong Xu, & Yongwu Peng. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00388
IEEE [1] Peng Jin, Chenglong Guo, Jiahao Li, Dejun Zhou, Guodong Xu, and Yongwu Peng, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00388. keywords: {covalent organic frameworks;aggregationinduced emission;molecular rotor;volatile organic compounds;chemical sensing}