Magnetically Tunable Transmissibility for Magneto-Responsive Elastomers Consisting of Magnetic and Nonmagnetic Particles AITranslate

Niigata University; Niigata University; Niigata University; Kanazawa University; Niigata University; Niigata University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Vibration experiments were performed for a bimodal magneto-responsive elastomer containing magnetic and nonmagnetic particles with thicknesses of 5 and 10 mm to investigate the effect of nonmagnetic particles on the natural frequency and the vibration transmissibility. The vibration experiments were carried out in a frequency range of 50–400 Hz at magnetic fields up to 80 mT. The frequency spectra of transmissibility at 0 mT for the bimodal elastomer showed a natural frequency in a frequency range of 50–150 Hz. The natural frequency shifted to higher frequencies as the magnetic field was raised. The maximum change in the natural frequency for the bimodal elastomer was 224 Hz, which was twice that for a monomodal elastomer filled only with magnetic particles (112 Hz). A proportional relationship was found between the change in natural frequency and the change in storage modulus in the linear viscoelastic regime for both monomodal and bimodal elastomers. A proportional relationship was also found between the natural frequency and the value of (G/m)1/2. It was found that the proportionality constant for the magnetic elastomer with a sample thickness of 10 mm was close to the calculated value. Furthermore, a demonstration of the electrical vibration control using the bimodal elastomer was presented.

KeyWords AITranslate

Magnetoresponsive elastomer magnetic elastomer magnetic gel stimuliresponsive material soft material Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00181

Chinese Library Classification Number:

Citation Information:

Vibration experiments were performed for a bimodal magneto-responsive elastomer containing magnetic and nonmagnetic particles with thicknesses of 5 and 10 mm to investigate the effect of nonmagnetic particles on the natural frequency and the vibration transmissibility. The vibration experiments were carried out in a frequency range of 50–400 Hz at magnetic fields up to 80 mT. The frequency spectra of transmissibility at 0 mT for the bimodal elastomer showed a natural frequency in a frequency range of 50–150 Hz. The natural frequency shifted to higher frequencies as the magnetic field was raised. The maximum change in the natural frequency for the bimodal elastomer was 224 Hz, which was twice that for a monomodal elastomer filled only with magnetic particles (112 Hz). A proportional relationship was found between the change in natural frequency and the change in storage modulus in the linear viscoelastic regime for both monomodal and bimodal elastomers. A proportional relationship was also found between the natural frequency and the value of (G/m)1/2. It was found that the proportionality constant for the magnetic elastomer with a sample thickness of 10 mm was close to the calculated value. Furthermore, a demonstration of the electrical vibration control using the bimodal elastomer was presented.

quote

GB/T 7714-2015 [1] Kejun Chen, Kazushi Nagashima, Shuya Takahashi, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00181.
MLA [1] Kejun Chen, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00181.
APA [1] Kejun Chen, Kazushi Nagashima, Shuya Takahashi, Toshihiko Komatsuzaki, Mika Kawai, & Tetsu Mitsumata. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00181
IEEE [1] Kejun Chen, Kazushi Nagashima, Shuya Takahashi, Toshihiko Komatsuzaki, Mika Kawai, and Tetsu Mitsumata, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00181. keywords: {Magnetoresponsive elastomer;magnetic elastomer;magnetic gel;stimuliresponsive material;soft material;Show More}