New Opportunities for Functional Materials from Metal Phosphonates AITranslate

King Abdullah University of Science and Technology (KAUST); Nankai University; King Abdullah University of Science and Technology (KAUST)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Hybrid functional materials and their derivatives are propelling a technological revolution in chemistry, materials science, and other disciplines. The performance of hybrid materials touches many fundamental aspects of energy conversion and storage, sustainable environment, and life sciences. Based on their rich chemistry, diverse metal phosphonates and their derivatives can be synthesized. These materials manifest various structures and enable new functionalities, which are hardly attainable in simple mixtures or other multicomponent materials. Here, we highlight and discuss the fascinating materials design innovations that organophosphonates can enable, with an eye on energy, environment, and biological applications.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.0c00095

Chinese Library Classification Number:

Citation Information:

Hybrid functional materials and their derivatives are propelling a technological revolution in chemistry, materials science, and other disciplines. The performance of hybrid materials touches many fundamental aspects of energy conversion and storage, sustainable environment, and life sciences. Based on their rich chemistry, diverse metal phosphonates and their derivatives can be synthesized. These materials manifest various structures and enable new functionalities, which are hardly attainable in simple mixtures or other multicomponent materials. Here, we highlight and discuss the fascinating materials design innovations that organophosphonates can enable, with an eye on energy, environment, and biological applications.

quote

GB/T 7714-2015 [1] YunPei Zhu, ZhongYong Yuan, Husam N. Alshareef. ACS Materials Letters, 2020(2). DOI:10.1021/acsmaterialslett.0c00095.
MLA [1] YunPei Zhu, et al., ACS Materials Letters, no. 2, 2020, https://doi.org/10.1021/acsmaterialslett.0c00095.
APA [1] YunPei Zhu, ZhongYong Yuan, & Husam N. Alshareef. (2020). ACS Materials Letters(2). https://doi.org/10.1021/acsmaterialslett.0c00095
IEEE [1] YunPei Zhu, ZhongYong Yuan, and Husam N. Alshareef, ACS Materials Letters, no. 2, 2020, doi: 10.1021/acsmaterialslett.0c00095.