University of the Basque Country UPV/EHU; University of the Basque Country UPV/EHU; University of the Basque Country UPV/EHU; University of the Basque Country UPV/EHU; Université de Haute-Alsace; Université de Haute-Alsace; University of Freiburg; University of Freiburg; University of Freiburg; University of the Basque Country UPV/EHU
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A complex crystallization behavior was observed for the alternating copolymer DMDS-alt-DVE synthesized via thiol–ene step-growth polymerization. Understanding the underlying complex crystallization processes of such innovative polythioethers is critical for their application, for example, in polymer coating technologies. These alternating copolymers have polymorphic traits, resulting in different phases that may display distinct crystalline structures. The copolymer DMDS-alt-DVE was studied in an earlier work, where only two crystalline phases were reported: a low melting, L – Tm, and high melting, H – Tm phase. Remarkably, the H – Tm form was only achieved by the previous formation and melting of the L – Tm form. We applied calorimetric techniques encompassing seven orders of magnitude in scanning rates to further explore this complex polymorphic behavior. Most importantly, by rapidly quenching the sample to temperatures well below room temperature, we detected an additional polymorphic form (characterized by a very low melting phase, denoted VL – Tm). Moreover, through tailored thermal protocols, we successfully produced samples containing only one, two, or all three polymorphs, providing insights into their interrelationships. Understanding polymorphism, crystallization, and the resulting morphological differences can have significant implications and potential impact on mechanical resistance and barrier properties.

KeyWords AITranslate

polymorphism polythioethers crystallization fast scanning chip calorimetry microcalorimetry
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00684

Chinese Library Classification Number:

Citation Information:

A complex crystallization behavior was observed for the alternating copolymer DMDS-alt-DVE synthesized via thiol–ene step-growth polymerization. Understanding the underlying complex crystallization processes of such innovative polythioethers is critical for their application, for example, in polymer coating technologies. These alternating copolymers have polymorphic traits, resulting in different phases that may display distinct crystalline structures. The copolymer DMDS-alt-DVE was studied in an earlier work, where only two crystalline phases were reported: a low melting, L – Tm, and high melting, H – Tm phase. Remarkably, the H – Tm form was only achieved by the previous formation and melting of the L – Tm form. We applied calorimetric techniques encompassing seven orders of magnitude in scanning rates to further explore this complex polymorphic behavior. Most importantly, by rapidly quenching the sample to temperatures well below room temperature, we detected an additional polymorphic form (characterized by a very low melting phase, denoted VL – Tm). Moreover, through tailored thermal protocols, we successfully produced samples containing only one, two, or all three polymorphs, providing insights into their interrelationships. Understanding polymorphism, crystallization, and the resulting morphological differences can have significant implications and potential impact on mechanical resistance and barrier properties.

quote

GB/T 7714-2015 [1] Valentina Pirela, Justine Elgoyhen, Radmila Tomovska, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00684.
MLA [1] Valentina Pirela, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00684.
APA [1] Valentina Pirela, Justine Elgoyhen, Radmila Tomovska, Jaime Martín, Cuong Minh Quoc Le, Abraham Chemtob, Brahim Bessif, Barbara Heck, Günter Reiter, & Alejandro J. Müller. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00684
IEEE [1] Valentina Pirela, Justine Elgoyhen, Radmila Tomovska, Jaime Martín, Cuong Minh Quoc Le, Abraham Chemtob, Brahim Bessif, Barbara Heck, Günter Reiter, and Alejandro J. Müller, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00684. keywords: {polymorphism;polythioethers;crystallization;fast scanning chip calorimetry;microcalorimetry}