daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

MAPbI3 Single Crystals Free from Hole-Trapping Centers for Enhanced Photodetectivity AITranslate

King Abdullah University of Science and Technology; King Abdullah University of Science and Technology; King Abdullah University of Science and Technology; King Abdullah University of Science and Technology; King Abdullah University of Science and Technology; King Abdullah University of Science and Technology;Saudi Aramco Research & Development Center, Dhahran 31311;Saudi Aramco Research & Development Center, Dhahran 31311; King Abdullah University of Science and Technology; King Abdullah University of Science and Technology; King Abdullah University of Science and Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Perovskite single crystals (PSCs) are considered the next breakthrough in optoelectronics research due to their free-grain boundary and much lower density of trap states compared to those of their polycrystalline counterparts. However, the inevitable formation of triiodide-based intrinsic defects during high-temperature crystal growth is one of the major challenges impeding the further development of optoelectronic devices based on PSCs. Here, we not only identified the existence of these triiodide ions as hole-trapping centers and their tremendous negative impact on the performance of PSCs, but more importantly, we used a reduction treatment to prevent their formation during crystal growth. The removal of such defect centers resulted in much higher charge carrier mobility and longer carrier lifetime than the untreated counterparts, leading to enhanced photodetection properties. The I3–-free MAPbI3 single crystal (MSC) devices consistently generated a more than 100 times higher photocurrent than that generated by I3–-rich devices under the same light intensity.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b01956

Chinese Library Classification Number:

Citation Information:

Perovskite single crystals (PSCs) are considered the next breakthrough in optoelectronics research due to their free-grain boundary and much lower density of trap states compared to those of their polycrystalline counterparts. However, the inevitable formation of triiodide-based intrinsic defects during high-temperature crystal growth is one of the major challenges impeding the further development of optoelectronic devices based on PSCs. Here, we not only identified the existence of these triiodide ions as hole-trapping centers and their tremendous negative impact on the performance of PSCs, but more importantly, we used a reduction treatment to prevent their formation during crystal growth. The removal of such defect centers resulted in much higher charge carrier mobility and longer carrier lifetime than the untreated counterparts, leading to enhanced photodetection properties. The I3–-free MAPbI3 single crystal (MSC) devices consistently generated a more than 100 times higher photocurrent than that generated by I3–-rich devices under the same light intensity.

quote

GB/T 7714-2015 [1] Chen Yang, Jehad K. ElDemellawi, Jun Yin, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b01956.
MLA [1] Chen Yang, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b01956.
APA [1] Chen Yang, Jehad K. ElDemellawi, Jun Yin, Dhinesh Babu Velusamy, AbdulHamid M. Emwas, Ahmed M. ElZohry, Issam Gereige, Ahmed AlSaggaf, Osman M. Bakr, Husam N. Alshareef, & Omar F. Mohammed. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b01956
IEEE [1] Chen Yang, Jehad K. ElDemellawi, Jun Yin, Dhinesh Babu Velusamy, AbdulHamid M. Emwas, Ahmed M. ElZohry, Issam Gereige, Ahmed AlSaggaf, Osman M. Bakr, Husam N. Alshareef, and Omar F. Mohammed, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b01956.